Standing and sitting adlayers in atomic layer deposition of ZnO
Journal Article
·
· Journal of Vacuum Science & Technology A: Vacuum, Surfaces, and Films
- Department of Mechanical Engineering & Material Science, Washington University in St. Louis, Missouri 63130 and Institute of Materials Science & Engineering, Washington University in St. Louis, Missouri 63130
- Department of Mechanical Engineering & Material Science, Washington University in St. Louis, Missouri 63130
- Department of Physics, Washington University in St. Louis, Missouri 63130
- SAFC Hitech, 1429 Hilldale Ave., Haverhill, Massachusetts 01832
- Institute of Materials Science & Engineering, Washington University in St. Louis, Missouri 63130 and Department of Physics, Washington University in St. Louis, Missouri 63130
Not Available
- Sponsoring Organization:
- USDOE
- Grant/Contract Number:
- AC36-08GO28308
- OSTI ID:
- 1421136
- Journal Information:
- Journal of Vacuum Science & Technology A: Vacuum, Surfaces, and Films, Journal Name: Journal of Vacuum Science & Technology A: Vacuum, Surfaces, and Films Journal Issue: 1 Vol. 34; ISSN 0734-2101; ISSN JVTAD6
- Publisher:
- American Vacuum SocietyCopyright Statement
- Country of Publication:
- United States
- Language:
- English
Similar Records
Standing and sitting adlayers in atomic layer deposition of ZnO
Hydroquinone-ZnO nano-laminate deposited by molecular-atomic layer deposition
Atomic layer deposition of ZnO on Cu-nanoclusters for methanol synthesis
Journal Article
·
2016
· Journal of Vacuum Science and Technology. A, Vacuum, Surfaces and Films
·
OSTI ID:22489775
+4 more
Hydroquinone-ZnO nano-laminate deposited by molecular-atomic layer deposition
Journal Article
·
2015
· Applied Physics Letters
·
OSTI ID:22398779
+3 more
Atomic layer deposition of ZnO on Cu-nanoclusters for methanol synthesis
Journal Article
·
2012
· Journal of Vacuum Science and Technology. A, Vacuum, Surfaces and Films
·
OSTI ID:1382021
+4 more