Title: Nanoindentation and in situ microcompression in different dose regimes of proton beam irradiated 304 SS

Authors:
; ORCiD logo ; ; ; ; ; ; ; ;
Publication Date:
Grant/Contract Number:
AC02-05CH11231
Type:
Publisher's Accepted Manuscript
Journal Name:
Journal of Nuclear Materials
Additional Journal Information:
Journal Volume: 486; Journal Issue: C; Related Information: CHORUS Timestamp: 2018-09-04 19:20:35; Journal ID: ISSN 0022-3115
Publisher:
Elsevier
Sponsoring Org:
USDOE
Country of Publication:
Netherlands
Language:
English
OSTI Identifier:
1419389

Reichardt, A., Lupinacci, A., Frazer, D., Bailey, N., Vo, H., Howard, C., Jiao, Z., Minor, A. M., Chou, P., and Hosemann, P.. Nanoindentation and in situ microcompression in different dose regimes of proton beam irradiated 304 SS. Netherlands: N. p., Web. doi:10.1016/j.jnucmat.2017.01.036.
Reichardt, A., Lupinacci, A., Frazer, D., Bailey, N., Vo, H., Howard, C., Jiao, Z., Minor, A. M., Chou, P., & Hosemann, P.. Nanoindentation and in situ microcompression in different dose regimes of proton beam irradiated 304 SS. Netherlands. doi:10.1016/j.jnucmat.2017.01.036.
Reichardt, A., Lupinacci, A., Frazer, D., Bailey, N., Vo, H., Howard, C., Jiao, Z., Minor, A. M., Chou, P., and Hosemann, P.. 2017. "Nanoindentation and in situ microcompression in different dose regimes of proton beam irradiated 304 SS". Netherlands. doi:10.1016/j.jnucmat.2017.01.036.
@article{osti_1419389,
title = {Nanoindentation and in situ microcompression in different dose regimes of proton beam irradiated 304 SS},
author = {Reichardt, A. and Lupinacci, A. and Frazer, D. and Bailey, N. and Vo, H. and Howard, C. and Jiao, Z. and Minor, A. M. and Chou, P. and Hosemann, P.},
abstractNote = {},
doi = {10.1016/j.jnucmat.2017.01.036},
journal = {Journal of Nuclear Materials},
number = C,
volume = 486,
place = {Netherlands},
year = {2017},
month = {4}
}