Title: Homogenization kinetics of a nickel-based superalloy produced by powder bed fusion laser sintering

Authors:
; ; ; ; ; ; ; ;
Publication Date:
Grant/Contract Number:
AC02-06CH11357
Type:
Publisher's Accepted Manuscript
Journal Name:
Scripta Materialia
Additional Journal Information:
Journal Volume: 131; Journal Issue: C; Related Information: CHORUS Timestamp: 2018-09-04 16:59:13; Journal ID: ISSN 1359-6462
Publisher:
Elsevier
Sponsoring Org:
USDOE
Country of Publication:
United States
Language:
English
OSTI Identifier:
1415242

Zhang, Fan, Levine, Lyle E., Allen, Andrew J., Campbell, Carelyn E., Lass, Eric A., Cheruvathur, Sudha, Stoudt, Mark R., Williams, Maureen E., and Idell, Yaakov. Homogenization kinetics of a nickel-based superalloy produced by powder bed fusion laser sintering. United States: N. p., Web. doi:10.1016/j.scriptamat.2016.12.037.
Zhang, Fan, Levine, Lyle E., Allen, Andrew J., Campbell, Carelyn E., Lass, Eric A., Cheruvathur, Sudha, Stoudt, Mark R., Williams, Maureen E., & Idell, Yaakov. Homogenization kinetics of a nickel-based superalloy produced by powder bed fusion laser sintering. United States. doi:10.1016/j.scriptamat.2016.12.037.
Zhang, Fan, Levine, Lyle E., Allen, Andrew J., Campbell, Carelyn E., Lass, Eric A., Cheruvathur, Sudha, Stoudt, Mark R., Williams, Maureen E., and Idell, Yaakov. 2017. "Homogenization kinetics of a nickel-based superalloy produced by powder bed fusion laser sintering". United States. doi:10.1016/j.scriptamat.2016.12.037.
@article{osti_1415242,
title = {Homogenization kinetics of a nickel-based superalloy produced by powder bed fusion laser sintering},
author = {Zhang, Fan and Levine, Lyle E. and Allen, Andrew J. and Campbell, Carelyn E. and Lass, Eric A. and Cheruvathur, Sudha and Stoudt, Mark R. and Williams, Maureen E. and Idell, Yaakov},
abstractNote = {},
doi = {10.1016/j.scriptamat.2016.12.037},
journal = {Scripta Materialia},
number = C,
volume = 131,
place = {United States},
year = {2017},
month = {4}
}