Title: Mechanical behavior of rare‐earth orthophosphates near the monazite/xenotime boundary characterized by nanoindentation

Authors:
; ; ; ; ;
Publication Date:
Grant/Contract Number:
U2015B0008; AC52-06NA25396
Type:
Publisher's Accepted Manuscript
Journal Name:
Materials Science and Engineering. A, Structural Materials: Properties, Microstructure and Processing
Additional Journal Information:
Journal Name: Materials Science and Engineering. A, Structural Materials: Properties, Microstructure and Processing Journal Volume: 691 Journal Issue: C; Journal ID: ISSN 0921-5093
Publisher:
Elsevier
Sponsoring Org:
USDOE National Nuclear Security Administration (NNSA)
Country of Publication:
Netherlands
Language:
English
OSTI Identifier:
1414783

Wilkinson, Taylor M., Wu, Dong, Musselman, Matthew A., Li, Nan, Mara, Nathan, and Packard, Corinne E.. Mechanical behavior of rare‐earth orthophosphates near the monazite/xenotime boundary characterized by nanoindentation. Netherlands: N. p., Web. doi:10.1016/j.msea.2017.03.041.
Wilkinson, Taylor M., Wu, Dong, Musselman, Matthew A., Li, Nan, Mara, Nathan, & Packard, Corinne E.. Mechanical behavior of rare‐earth orthophosphates near the monazite/xenotime boundary characterized by nanoindentation. Netherlands. doi:10.1016/j.msea.2017.03.041.
Wilkinson, Taylor M., Wu, Dong, Musselman, Matthew A., Li, Nan, Mara, Nathan, and Packard, Corinne E.. 2017. "Mechanical behavior of rare‐earth orthophosphates near the monazite/xenotime boundary characterized by nanoindentation". Netherlands. doi:10.1016/j.msea.2017.03.041.
@article{osti_1414783,
title = {Mechanical behavior of rare‐earth orthophosphates near the monazite/xenotime boundary characterized by nanoindentation},
author = {Wilkinson, Taylor M. and Wu, Dong and Musselman, Matthew A. and Li, Nan and Mara, Nathan and Packard, Corinne E.},
abstractNote = {},
doi = {10.1016/j.msea.2017.03.041},
journal = {Materials Science and Engineering. A, Structural Materials: Properties, Microstructure and Processing},
number = C,
volume = 691,
place = {Netherlands},
year = {2017},
month = {4}
}