Title: Elastic and plastic deformations in a high entropy alloy investigated using a nanoindentation method

Authors:
ORCiD logo; ;
Publication Date:
Sponsoring Org.:
USDOE
OSTI Identifier:
1396318
Grant/Contract Number:  
NE0000693
Resource Type:
Publisher's Accepted Manuscript
Journal Name:
Intermetallics
Additional Journal Information:
Journal Name: Intermetallics Journal Volume: 68 Journal Issue: C; Journal ID: ISSN 0966-9795
Publisher:
Elsevier
Country of Publication:
United Kingdom
Language:
English

Citation Formats

Wu, D., Jang, J. S. C., and Nieh, T. G.. Elastic and plastic deformations in a high entropy alloy investigated using a nanoindentation method. United Kingdom: N. p., 2016. Web. https://doi.org/10.1016/j.intermet.2015.10.002.
Wu, D., Jang, J. S. C., & Nieh, T. G.. Elastic and plastic deformations in a high entropy alloy investigated using a nanoindentation method. United Kingdom. https://doi.org/10.1016/j.intermet.2015.10.002
Wu, D., Jang, J. S. C., and Nieh, T. G.. Fri . "Elastic and plastic deformations in a high entropy alloy investigated using a nanoindentation method". United Kingdom. https://doi.org/10.1016/j.intermet.2015.10.002.
@article{osti_1396318,
title = {Elastic and plastic deformations in a high entropy alloy investigated using a nanoindentation method},
author = {Wu, D. and Jang, J. S. C. and Nieh, T. G.},
abstractNote = {},
doi = {10.1016/j.intermet.2015.10.002},
journal = {Intermetallics},
number = C,
volume = 68,
place = {United Kingdom},
year = {2016},
month = {1}
}

Journal Article:
Free Publicly Available Full Text
Publisher's Version of Record
https://doi.org/10.1016/j.intermet.2015.10.002

Citation Metrics:
Cited by: 12 works
Citation information provided by
Web of Science

Save / Share: