Probing elastically or plastically induced structural heterogeneities in bulk metallic glasses by nanoindentation pop-in tests
Abstract
Shear banding dynamics in bulk metallic glasses (BMGs) is manifested by the spatiotemporal evolution of strain fields which in turn depend on structural heterogeneities. The spacing of these heterogeneities, as a characteristic length scale, was determined from the analysis of nanoindentation pop-in tests using a stochastic model. Furthermore, the pre-stress by elastic bending and residual stress by plastic bending of BMG plates were found to dramatically decrease such spacings, thus increasing heterogeneity density and mechanically rejuvenating the glass structure.
- Authors:
-
- Univ. of Tennessee, Knoxville, TN (United States). Dept. of Materials Science and Engineering
- Univ. of Tennessee, Knoxville, TN (United States). Dept. of Materials Science and Engineering; Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States). Materials Science and Technology Div.
- Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States). Materials Science and Technology Div.
- Publication Date:
- Research Org.:
- Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States)
- Sponsoring Org.:
- USDOE
- OSTI Identifier:
- 1376437
- Alternate Identifier(s):
- OSTI ID: 1375664
- Grant/Contract Number:
- AC05-00OR22725
- Resource Type:
- Accepted Manuscript
- Journal Name:
- AIP Advances
- Additional Journal Information:
- Journal Volume: 7; Journal Issue: 8; Journal ID: ISSN 2158-3226
- Publisher:
- American Institute of Physics (AIP)
- Country of Publication:
- United States
- Language:
- English
- Subject:
- 36 MATERIALS SCIENCE
Citation Formats
Liu, Tingkun, Gao, Yanfei, and Bei, Hongbin. Probing elastically or plastically induced structural heterogeneities in bulk metallic glasses by nanoindentation pop-in tests. United States: N. p., 2017.
Web. doi:10.1063/1.4993719.
Liu, Tingkun, Gao, Yanfei, & Bei, Hongbin. Probing elastically or plastically induced structural heterogeneities in bulk metallic glasses by nanoindentation pop-in tests. United States. https://doi.org/10.1063/1.4993719
Liu, Tingkun, Gao, Yanfei, and Bei, Hongbin. Fri .
"Probing elastically or plastically induced structural heterogeneities in bulk metallic glasses by nanoindentation pop-in tests". United States. https://doi.org/10.1063/1.4993719. https://www.osti.gov/servlets/purl/1376437.
@article{osti_1376437,
title = {Probing elastically or plastically induced structural heterogeneities in bulk metallic glasses by nanoindentation pop-in tests},
author = {Liu, Tingkun and Gao, Yanfei and Bei, Hongbin},
abstractNote = {Shear banding dynamics in bulk metallic glasses (BMGs) is manifested by the spatiotemporal evolution of strain fields which in turn depend on structural heterogeneities. The spacing of these heterogeneities, as a characteristic length scale, was determined from the analysis of nanoindentation pop-in tests using a stochastic model. Furthermore, the pre-stress by elastic bending and residual stress by plastic bending of BMG plates were found to dramatically decrease such spacings, thus increasing heterogeneity density and mechanically rejuvenating the glass structure.},
doi = {10.1063/1.4993719},
journal = {AIP Advances},
number = 8,
volume = 7,
place = {United States},
year = {Fri Jul 21 00:00:00 EDT 2017},
month = {Fri Jul 21 00:00:00 EDT 2017}
}
Free Publicly Available Full Text
Publisher's Version of Record
Other availability
Cited by: 4 works
Citation information provided by
Web of Science
Web of Science
Save to My Library
You must Sign In or Create an Account in order to save documents to your library.
Works referenced in this record:
Correlation between local elastic heterogeneities and overall elastic properties in metallic glasses
journal, December 2016
- Sun, B. A.; Hu, Y. C.; Wang, D. P.
- Acta Materialia, Vol. 121
Embrittlement of a bulk metallic glass due to low-temperature annealing
journal, July 2002
- Ramamurty, U.; Lee, M. L.; Basu, J.
- Scripta Materialia, Vol. 47, Issue 2
Radial distribution function and structural relaxation in amorphous solids
journal, December 1981
- Srolovitz, D.; Egami, T.; Vitek, V.
- Physical Review B, Vol. 24, Issue 12
Direct synchrotron x-ray measurements of local strain fields in elastically and plastically bent metallic glasses
journal, December 2015
- Wu, Y.; Stoica, A. D.; Ren, Y.
- Intermetallics, Vol. 67
On the correlation between microscopic structural heterogeneity and embrittlement behavior in metallic glasses
journal, October 2015
- Li, Weidong; Gao, Yanfei; Bei, Hongbin
- Scientific Reports, Vol. 5, Issue 1
The thermal history effect on shear band initiation in metallic glass
journal, June 2016
- Wang, S.; Ye, Y. F.; Shi, S. Q.
- Journal of Applied Physics, Vol. 119, Issue 24
Embrittlement of a bulk metallic glass due to sub- annealing
journal, March 2005
- Murali, P.; Ramamurty, U.
- Acta Materialia, Vol. 53, Issue 5
Deformation-induced spatiotemporal fluctuation, evolution and localization of strain fields in a bulk metallic glass
journal, August 2015
- Wu, Y.; Bei, H.; Wang, Y. L.
- International Journal of Plasticity, Vol. 71
Reflections from the glass maze
journal, December 2010
- Ma, Evan; Zhang, Ze
- Nature Materials, Vol. 10, Issue 1
Scale effects in convoluted thermal/spatial statistics of plasticity initiation in small stressed volumes during nanoindentation
journal, October 2012
- Li, T. L.; Bei, H.; Morris, J. R.
- Materials Science and Technology, Vol. 28, Issue 9-10
The role of configurational disorder on plastic and dynamic deformation in Cu64Zr36 metallic glasses: A molecular dynamics analysis
journal, January 2017
- Feng, S. D.; Chan, K. C.; Chen, S. H.
- Scientific Reports, Vol. 7, Issue 1
Density changes in shear bands of a metallic glass determined by correlative analytical transmission electron microscopy
journal, July 2014
- Rösner, Harald; Peterlechner, Martin; Kübel, Christian
- Ultramicroscopy, Vol. 142
Microstructural heterogeneity perspective on the yield strength of metallic glasses
journal, February 2016
- Cao, X. F.; Gao, M.; Zhao, L. Z.
- Journal of Applied Physics, Vol. 119, Issue 8
Structural heterogeneity induced plasticity in bulk metallic glasses: From well-relaxed fragile glass to metal-like behavior
journal, October 2013
- Li, Weidong; Bei, H.; Tong, Y.
- Applied Physics Letters, Vol. 103, Issue 17
Structural rejuvenation in bulk metallic glasses
journal, March 2015
- Tong, Y.; Iwashita, T.; Dmowski, W.
- Acta Materialia, Vol. 86
Strength statistics of single crystals and metallic glasses under small stressed volumes
journal, September 2016
- Gao, Yanfei; Bei, Hongbin
- Progress in Materials Science, Vol. 82
Stress-dependent shear transformation zone in Ni Nb thin film metallic glass and its correlation with deformation mode transition
journal, September 2016
- Wang, C.; Cao, Q. P.; Wang, X. D.
- Scripta Materialia, Vol. 122
Stress-induced structural transformation and shear banding during simulated nanoindentation of a metallic glass
journal, August 2007
- Shi, Yunfeng; Falk, Michael L.
- Acta Materialia, Vol. 55, Issue 13
How thermally activated deformation starts in metallic glass
journal, September 2014
- Fan, Yue; Iwashita, Takuya; Egami, Takeshi
- Nature Communications, Vol. 5, Issue 1
Local elastic properties of a metallic glass
journal, May 2011
- Wagner, Hannes; Bedorf, Dennis; Küchemann, Stefan
- Nature Materials, Vol. 10, Issue 6
Structural processes that initiate shear localization in metallic glass
journal, October 2009
- Cao, A. J.; Cheng, Y. Q.; Ma, E.
- Acta Materialia, Vol. 57, Issue 17
Rejuvenation decreases shear band sliding velocity in Pt-based metallic glasses
journal, January 2017
- Denis, P.; Meylan, C. M.; Ebner, C.
- Materials Science and Engineering: A, Vol. 684
Mechanical behavior of amorphous alloys
journal, July 2007
- Schuh, C.; Hufnagel, T.; Ramamurty, U.
- Acta Materialia, Vol. 55, Issue 12
Specimen Size Effects on Zr-Based Bulk Metallic Glasses Investigated by Uniaxial Compression and Spherical Nanoindentation
journal, September 2009
- Bei, H.; Lu, Z. P.; Shim, S.
- Metallurgical and Materials Transactions A, Vol. 41, Issue 7
Test environments and mechanical properties of Zr-base bulk amorphous alloys
journal, July 1998
- Liu, C. T.; Heatherly, L.; Horton, J. A.
- Metallurgical and Materials Transactions A, Vol. 29, Issue 7
Origin of embrittlement in metallic glasses
journal, August 2016
- Garrett, Glenn R.; Demetriou, Marios D.; Launey, Maximilien E.
- Proceedings of the National Academy of Sciences, Vol. 113, Issue 37
Experimental characterization of shear transformation zones for plastic flow of bulk metallic glasses
journal, September 2008
- Pan, D.; Inoue, A.; Sakurai, T.
- Proceedings of the National Academy of Sciences, Vol. 105, Issue 39
A microscopic mechanism for steady state inhomogeneous flow in metallic glasses
journal, April 1977
- Spaepen, Frans
- Acta Metallurgica, Vol. 25, Issue 4
Universal structural parameter to quantitatively predict metallic glass properties
journal, December 2016
- Ding, Jun; Cheng, Yong-Qiang; Sheng, Howard
- Nature Communications, Vol. 7, Issue 1
Plastic deformation in metallic glasses
journal, January 1979
- Argon, A. S.
- Acta Metallurgica, Vol. 27, Issue 1
Effects of flow defects on hypothetical ZrCu metallic glasses microstructure and plasticity: A molecular dynamics analysis
journal, January 2016
- Feng, S. D.; Qi, L.; Pan, S. P.
- Journal of Alloys and Compounds, Vol. 656
Tailoring structural inhomogeneities in metallic glasses to enable tensile ductility at room temperature
journal, December 2016
- Ma, E.; Ding, J.
- Materials Today, Vol. 19, Issue 10
Effect of residual stresses on the hardness of bulk metallic glasses
journal, April 2011
- Wang, L.; Bei, H.; Gao, Y. F.
- Acta Materialia, Vol. 59, Issue 7
Shear-banding Induced Indentation Size Effect in Metallic Glasses
journal, June 2016
- Lu, Y. M.; Sun, B. A.; Zhao, L. Z.
- Scientific Reports, Vol. 6, Issue 1
Intrinsic correlation between β-relaxation and spatial heterogeneity in a metallic glass
journal, May 2016
- Zhu, F.; Nguyen, H. K.; Song, S. X.
- Nature Communications, Vol. 7, Issue 1
Effect of residual stresses on the onset of yielding in a Zr-based metallic glass
journal, December 2011
- Wang, L.; Bei, H.; Gao, Y. F.
- Acta Materialia, Vol. 59, Issue 20