Effect of tip radius on the incipient plasticity of chromium studied by nanoindentation
Abstract
The onset of plasticity in Cr was investigated by nanoindentation using indenters with tip radii ranging from 60 to 759 nm. The stress for incipient plasticity was found to increase with decreasing tip radius. We find that the cumulative pop-in probability on load could be described successfully by a combined model over the full range of tip radius, indicating that the incipient plasticity might be triggered either by the homogeneous nucleation of dislocation or by the activation of existing dislocations underneath the indenter.
- Authors:
-
- Univ. of Tennessee, Knoxville, TN (United States). Dept. of Materials Science and Engineering
- Univ. of Tennessee, Knoxville, TN (United States). Dept. of Materials Science and Engineering; Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States). Materials Science & Technology Division
- Publication Date:
- Research Org.:
- Oak Ridge National Laboratory (ORNL), Oak Ridge, TN (United States)
- Sponsoring Org.:
- USDOE Office of Science (SC), Basic Energy Sciences (BES); National Science Foundation (NSF)
- OSTI Identifier:
- 1286763
- Alternate Identifier(s):
- OSTI ID: 1251509
- Grant/Contract Number:
- AC05-00OR22725; DMR-0905979
- Resource Type:
- Accepted Manuscript
- Journal Name:
- Scripta Materialia
- Additional Journal Information:
- Journal Volume: 94; Journal Issue: C; Journal ID: ISSN 1359-6462
- Publisher:
- Elsevier
- Country of Publication:
- United States
- Language:
- English
- Subject:
- 36 MATERIALS SCIENCE; Nanoindentation; Onset of yielding; Dislocation dynamics; Tip radius effect; Metallic material
Citation Formats
Wu, Dong, Morris, James R., and Nieh, T. G. Effect of tip radius on the incipient plasticity of chromium studied by nanoindentation. United States: N. p., 2014.
Web. doi:10.1016/j.scriptamat.2014.09.017.
Wu, Dong, Morris, James R., & Nieh, T. G. Effect of tip radius on the incipient plasticity of chromium studied by nanoindentation. United States. https://doi.org/10.1016/j.scriptamat.2014.09.017
Wu, Dong, Morris, James R., and Nieh, T. G. Wed .
"Effect of tip radius on the incipient plasticity of chromium studied by nanoindentation". United States. https://doi.org/10.1016/j.scriptamat.2014.09.017. https://www.osti.gov/servlets/purl/1286763.
@article{osti_1286763,
title = {Effect of tip radius on the incipient plasticity of chromium studied by nanoindentation},
author = {Wu, Dong and Morris, James R. and Nieh, T. G.},
abstractNote = {The onset of plasticity in Cr was investigated by nanoindentation using indenters with tip radii ranging from 60 to 759 nm. The stress for incipient plasticity was found to increase with decreasing tip radius. We find that the cumulative pop-in probability on load could be described successfully by a combined model over the full range of tip radius, indicating that the incipient plasticity might be triggered either by the homogeneous nucleation of dislocation or by the activation of existing dislocations underneath the indenter.},
doi = {10.1016/j.scriptamat.2014.09.017},
journal = {Scripta Materialia},
number = C,
volume = 94,
place = {United States},
year = {Wed Oct 01 00:00:00 EDT 2014},
month = {Wed Oct 01 00:00:00 EDT 2014}
}
Free Publicly Available Full Text
Publisher's Version of Record
Other availability
Cited by: 34 works
Citation information provided by
Web of Science
Web of Science
Save to My Library
You must Sign In or Create an Account in order to save documents to your library.
Works referenced in this record:
Plasticity in small-sized metallic systems: Intrinsic versus extrinsic size effect
journal, August 2011
- Greer, Julia R.; De Hosson, Jeff Th. M.
- Progress in Materials Science, Vol. 56, Issue 6
Tensile and compressive behavior of tungsten, molybdenum, tantalum and niobium at the nanoscale
journal, April 2010
- Kim, Ju-Young; Jang, Dongchan; Greer, Julia R.
- Acta Materialia, Vol. 58, Issue 7
Plasticity of bcc micropillars controlled by competition between dislocation multiplication and depletion
journal, May 2013
- Ryu, Ill; Nix, William D.; Cai, Wei
- Acta Materialia, Vol. 61, Issue 9
Correlation between dislocation density and nanomechanical response during nanoindentation
journal, February 2012
- Barnoush, Afrooz
- Acta Materialia, Vol. 60, Issue 3
Microstructure versus Size: Mechanical Properties of Electroplated Single Crystalline Cu Nanopillars
journal, April 2010
- Jennings, Andrew T.; Burek, Michael J.; Greer, Julia R.
- Physical Review Letters, Vol. 104, Issue 13
Determining the activation energy and volume for the onset of plasticity during nanoindentation
journal, February 2006
- Mason, J. K.; Lund, A. C.; Schuh, C. A.
- Physical Review B, Vol. 73, Issue 5
The effect of crystal orientation on the stochastic behavior of dislocation nucleation and multiplication during nanoindentation
journal, March 2013
- Salehinia, I.; Lawrence, S. K.; Bahr, D. F.
- Acta Materialia, Vol. 61, Issue 5
Effect of solid solution elements on nanoindentation hardness, rate dependence, and incipient plasticity in fine grained magnesium alloys
journal, December 2011
- Somekawa, Hidetoshi; Schuh, Christopher A.
- Acta Materialia, Vol. 59, Issue 20
Dislocation Nucleation and Source Activation during Nanoindentation Yield Points
journal, July 2007
- Zbib, A. A.; Bahr, D. F.
- Metallurgical and Materials Transactions A, Vol. 38, Issue 13
Temperature dependence of the plastic flow behavior of tantalum
journal, January 2010
- Rajulapati†, K. V.; Biener, M. M.; Biener, J.
- Philosophical Magazine Letters, Vol. 90, Issue 1
Dislocation nucleation in bcc Ta single crystals studied by nanoindentation
journal, October 2007
- Biener, Monika M.; Biener, Juergen; Hodge, Andrea M.
- Physical Review B, Vol. 76, Issue 16
Incipient plasticity and dislocation nucleation of FeCoCrNiMn high-entropy alloy
journal, May 2013
- Zhu, C.; Lu, Z. P.; Nieh, T. G.
- Acta Materialia, Vol. 61, Issue 8
Time-dependent incipient plasticity in Ni 3 Al as observed in nanoindentation
journal, February 2005
- Wo, P. C.; Zuo, L.; Ngan, A. H. W.
- Journal of Materials Research, Vol. 20, Issue 2
A different type of indentation size effect
journal, November 2008
- Shim, S.; Bei, H.; George, E. P.
- Scripta Materialia, Vol. 59, Issue 10
Strength differences arising from homogeneous versus heterogeneous dislocation nucleation
journal, February 2008
- Bei, H.; Gao, Y. F.; Shim, S.
- Physical Review B, Vol. 77, Issue 6
Size Effects and Stochastic Behavior of Nanoindentation Pop In
journal, April 2011
- Morris, J. R.; Bei, H.; Pharr, G. M.
- Physical Review Letters, Vol. 106, Issue 16
Dislocation mechanisms of radius effect on displacement bursts during spherical nanoindentations
journal, June 2012
- Shin, Chansun; Shim, Sanghoon
- Journal of Materials Research, Vol. 27, Issue 16
Scale effects in convoluted thermal/spatial statistics of plasticity initiation in small stressed volumes during nanoindentation
journal, October 2012
- Li, T. L.; Bei, H.; Morris, J. R.
- Materials Science and Technology, Vol. 28, Issue 9-10
Incipient plasticity and dislocation nucleation in body-centered cubic chromium
journal, July 2014
- Wu, D.; Nieh, T. G.
- Materials Science and Engineering: A, Vol. 609
Dislocation Substructures in Deformed and Recovered Chromium
journal, January 1964
- McLaren, Ac
- Australian Journal of Physics, Vol. 17, Issue 4
A Statistical Distribution Function of Wide Applicability
journal, September 1951
- Weibull, Waloddi
- Journal of Applied Mechanics, Vol. 18, Issue 3
A stochastic model for the size dependence of spherical indentation pop-in
journal, September 2013
- Sudharshan Phani, P.; Johanns, Kurt E.; George, Easo P.
- Journal of Materials Research, Vol. 28, Issue 19
Grain-boundary strengthening in nanocrystalline chromium and the Hall–Petch coefficient of body-centered cubic metals
journal, January 2013
- Wu, D.; Zhang, Junyan; Huang, J. C.
- Scripta Materialia, Vol. 68, Issue 2
Works referencing / citing this record:
Materials and Corrosion Trends in Offshore and Subsea Oil and Gas Production
text, January 2017
- Iannuzzi, Mariano; Barnoush, Afrooz; Johnsen, Roy
- engrXiv
Materials and Corrosion Trends in Offshore and Subsea Oil and Gas Production
posted_content, April 2017
- Iannuzzi, Mariano; Barnoush, Afrooz; Johnsen, Roy
Materials and corrosion trends in offshore and subsea oil and gas production
journal, July 2017
- Iannuzzi, Mariano; Barnoush, Afrooz; Johnsen, Roy
- npj Materials Degradation, Vol. 1, Issue 1