Title: Electrocatalysts by atomic layer deposition for fuel cell applications

Here, fuel cells are a promising technology solution for reliable and clean energy because they offer high energy conversion efficiency and low emission of pollutants. However, high cost and insufficient durability are considerable challenges for widespread adoption of polymer electrolyte membrane fuel cells (PEMFCs) in practical applications. Current PEMFCs catalysts have been identified as major contributors to both the high cost and limited durability. Atomic layer deposition (ALD) is emerging as a powerful technique for solving these problems due to its exclusive advantages over other methods. In this review, we summarize recent developments of ALD in PEMFCs with a focus on design of materials for improved catalyst activity and durability. New research directions and future trends have also been discussed.
Authors:
 [1] ;  [2] ;  [2] ;  [1]
  1. Univ. of Western Ontario, London, ON (Canada)
  2. Pacific Northwest National Lab. (PNNL), Richland, WA (United States)
Publication Date:
Grant/Contract Number:
AC05-76RL01830; KC020105-FWP12152
Type:
Accepted Manuscript
Journal Name:
Nano Energy
Additional Journal Information:
Journal Volume: 117; Journal Issue: C; Journal ID: ISSN 2211-2855
Publisher:
Elsevier
Research Org:
Pacific Northwest National Lab. (PNNL), Richland, WA (United States)
Sponsoring Org:
USDOE
Country of Publication:
United States
Language:
English
Subject:
37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CHEMISTRY; atomic layer deposition; fuel cells; electrocatalysts; nanomaterials; catalyst design
OSTI Identifier:
1250868
Alternate Identifier(s):
OSTI ID: 1419556

Cheng, Niancai, Shao, Yuyan, Liu, Jun, and Sun, Xueliang. Electrocatalysts by atomic layer deposition for fuel cell applications. United States: N. p., Web. doi:10.1016/j.nanoen.2016.01.016.
Cheng, Niancai, Shao, Yuyan, Liu, Jun, & Sun, Xueliang. Electrocatalysts by atomic layer deposition for fuel cell applications. United States. doi:10.1016/j.nanoen.2016.01.016.
Cheng, Niancai, Shao, Yuyan, Liu, Jun, and Sun, Xueliang. 2016. "Electrocatalysts by atomic layer deposition for fuel cell applications". United States. doi:10.1016/j.nanoen.2016.01.016. https://www.osti.gov/servlets/purl/1250868.
@article{osti_1250868,
title = {Electrocatalysts by atomic layer deposition for fuel cell applications},
author = {Cheng, Niancai and Shao, Yuyan and Liu, Jun and Sun, Xueliang},
abstractNote = {Here, fuel cells are a promising technology solution for reliable and clean energy because they offer high energy conversion efficiency and low emission of pollutants. However, high cost and insufficient durability are considerable challenges for widespread adoption of polymer electrolyte membrane fuel cells (PEMFCs) in practical applications. Current PEMFCs catalysts have been identified as major contributors to both the high cost and limited durability. Atomic layer deposition (ALD) is emerging as a powerful technique for solving these problems due to its exclusive advantages over other methods. In this review, we summarize recent developments of ALD in PEMFCs with a focus on design of materials for improved catalyst activity and durability. New research directions and future trends have also been discussed.},
doi = {10.1016/j.nanoen.2016.01.016},
journal = {Nano Energy},
number = C,
volume = 117,
place = {United States},
year = {2016},
month = {1}
}