Title: Catalyst synthesis and evaluation using an integrated atomic layer deposition synthesis–catalysis testing tool

Authors:
 [1];  [1];  [2];  [3];  [3];  [3]; ORCiD logo [1];  [4];  [5]
  1. Chemical Sciences and Engineering Division, Argonne National Laboratory, Lemont, Illinois 60439, USA
  2. Chemical Sciences and Engineering Division, Argonne National Laboratory, Lemont, Illinois 60439, USA, Department of Chemical Engineering, University of Illinois at Chicago, Chicago, Illinois 60607, USA
  3. Arradiance Inc., Sudbury, Massachusetts 01776, USA
  4. Chemical Sciences and Engineering Division, Argonne National Laboratory, Lemont, Illinois 60439, USA, Department of Chemistry, Illinois Institute of Technology, Chicago, Illinois 60616, USA
  5. Chemical Sciences and Engineering Division, Argonne National Laboratory, Lemont, Illinois 60439, USA, Department of Chemistry, Northwestern University, Evanston, Illinois 60208, USA
Publication Date:
Sponsoring Org.:
USDOE
OSTI Identifier:
1229634
Grant/Contract Number:  
AC-02-06H11357
Resource Type:
Publisher's Accepted Manuscript
Journal Name:
Review of Scientific Instruments
Additional Journal Information:
Journal Name: Review of Scientific Instruments Journal Volume: 86 Journal Issue: 8; Journal ID: ISSN 0034-6748
Publisher:
American Institute of Physics
Country of Publication:
United States
Language:
English

Citation Formats

Camacho-Bunquin, Jeffrey, Shou, Heng, Aich, Payoli, Beaulieu, David R., Klotzsch, Helmut, Bachman, Stephen, Marshall, Christopher L., Hock, Adam, and Stair, Peter. Catalyst synthesis and evaluation using an integrated atomic layer deposition synthesis–catalysis testing tool. United States: N. p., 2015. Web. doi:10.1063/1.4928614.
Camacho-Bunquin, Jeffrey, Shou, Heng, Aich, Payoli, Beaulieu, David R., Klotzsch, Helmut, Bachman, Stephen, Marshall, Christopher L., Hock, Adam, & Stair, Peter. Catalyst synthesis and evaluation using an integrated atomic layer deposition synthesis–catalysis testing tool. United States. doi:10.1063/1.4928614.
Camacho-Bunquin, Jeffrey, Shou, Heng, Aich, Payoli, Beaulieu, David R., Klotzsch, Helmut, Bachman, Stephen, Marshall, Christopher L., Hock, Adam, and Stair, Peter. Mon . "Catalyst synthesis and evaluation using an integrated atomic layer deposition synthesis–catalysis testing tool". United States. doi:10.1063/1.4928614.
@article{osti_1229634,
title = {Catalyst synthesis and evaluation using an integrated atomic layer deposition synthesis–catalysis testing tool},
author = {Camacho-Bunquin, Jeffrey and Shou, Heng and Aich, Payoli and Beaulieu, David R. and Klotzsch, Helmut and Bachman, Stephen and Marshall, Christopher L. and Hock, Adam and Stair, Peter},
abstractNote = {},
doi = {10.1063/1.4928614},
journal = {Review of Scientific Instruments},
number = 8,
volume = 86,
place = {United States},
year = {2015},
month = {8}
}

Journal Article:
Free Publicly Available Full Text
Publisher's Version of Record
DOI: 10.1063/1.4928614

Citation Metrics:
Cited by: 7 works
Citation information provided by
Web of Science

Save / Share:

Works referenced in this record:

Atomic Layer Deposition of Ir−Pt Alloy Films
journal, April 2010

  • Christensen, Steven T.; Elam, Jeffrey W.
  • Chemistry of Materials, Vol. 22, Issue 8, p. 2517-2525
  • DOI: 10.1021/cm9031978

Atomic Layer Deposition: An Overview
journal, January 2010

  • George, Steven M.
  • Chemical Reviews, Vol. 110, Issue 1, p. 111-131
  • DOI: 10.1021/cr900056b

Atomic Layer Deposition of Platinum Thin Films
journal, May 2003

  • Aaltonen, Titta; Ritala, Mikko; Sajavaara, Timo
  • Chemistry of Materials, Vol. 15, Issue 9, p. 1924-1928
  • DOI: 10.1021/cm021333t