SELECTION OF PROCESS TUBES FOR REPLACEMENT AT F REACTOR
Author(s):
Subject Terms:
100 AreasCOOLANT LEAKAGEF ReactorHANFORD PRODUCTION REACTORSMetallurgyReactor TechnologyTUBE CORROSION
Document Location:
DOE Public Reading Room - Hanford Battelle P.O. Box 999 MS H2-53 Richland WA 99352 (509)372-7443
Document Type:
REPORT
Publication Date:
1956 Mar 05
Declassification Date:
1981 Jul 13
Declassification Status:
Declassified
Document Pages:
6
Accession Number:
RL-1-363394
Document Number(s):
HW-41804
Originating Research Org.:
GE - HAPO
OpenNet Entry Date:
2004 Feb 24
OpenNet Modified Date:
2015 Aug 28
Description/Abstract:
PRESENTS AN ANALYSIS OF THE PROCESS TUBE SITUATION AT F REACTOR AND SUGGEST THAT TUBES BE SCHEDULED FOR REPLACEMENT WHEN THE CALCULATED RESIDUAL TUBE WALL THICKNESS IS 35 MILS ON THE NEAR SIDE AND 25 MILS ON THE FAR SIDE, THE LOW PH PROCESS WATER SUPPLIED TO THE FAR SIDE OF F REACTOR UNDER PT-S HAS APPRECIABLY REDUCED THE AL CORROSION RATE ON THAT SIDE.