Abstract
The techniques and the results of studies of the mechanical properties of brown coal discovered in a zone adjacent to the location of the Rogowiec power plant (Poland) are described. The studies were conducted by the geotechnical laboratory of the Polytechnical Institute in the city of Lodz. Included in the program of studies were: tests of the brown coal (eight samples with a diameter to height ratio of d/h = 10.0/7.5; 11.1/7.8; 9.3/8.8; 8.1/6.8; 8.5/9.4; 8.0/8.8; 7.9/7.6 adn 8.8/8.6; dimensions in centimeters) for single axis compression (destroying stress was found to be 0.778; 0.660; 0.376; 0.804; 0.140; 0.472; 0.408 and 0.278 MPa); tests of samples (five units) for shear strength (the chip force is 0.36; 0.46; 0.39; 0.11 and 0.36 kilonewtons); tests of the samples (two samples, both with a diameter of 3.8 cm and a height of 7.6 cm) for stretching (the destructive force is 50.1 and 54.9 kilonewtons); odometric tests to determine the odometric modulus of compressibility of the brown coal (a total of four samples; three of which were loaded by a force in the range of 0.6-1.2 MPa and one in the range of 0-1.1 MPa; the odometric modulus of compressibility is in the range of
More>>
Citation Formats
Okruszek, Z.
Study of the mechanical properties of brown coal.
Poland: N. p.,
1980.
Web.
Okruszek, Z.
Study of the mechanical properties of brown coal.
Poland.
Okruszek, Z.
1980.
"Study of the mechanical properties of brown coal."
Poland.
@misc{etde_5805187,
title = {Study of the mechanical properties of brown coal}
author = {Okruszek, Z}
abstractNote = {The techniques and the results of studies of the mechanical properties of brown coal discovered in a zone adjacent to the location of the Rogowiec power plant (Poland) are described. The studies were conducted by the geotechnical laboratory of the Polytechnical Institute in the city of Lodz. Included in the program of studies were: tests of the brown coal (eight samples with a diameter to height ratio of d/h = 10.0/7.5; 11.1/7.8; 9.3/8.8; 8.1/6.8; 8.5/9.4; 8.0/8.8; 7.9/7.6 adn 8.8/8.6; dimensions in centimeters) for single axis compression (destroying stress was found to be 0.778; 0.660; 0.376; 0.804; 0.140; 0.472; 0.408 and 0.278 MPa); tests of samples (five units) for shear strength (the chip force is 0.36; 0.46; 0.39; 0.11 and 0.36 kilonewtons); tests of the samples (two samples, both with a diameter of 3.8 cm and a height of 7.6 cm) for stretching (the destructive force is 50.1 and 54.9 kilonewtons); odometric tests to determine the odometric modulus of compressibility of the brown coal (a total of four samples; three of which were loaded by a force in the range of 0.6-1.2 MPa and one in the range of 0-1.1 MPa; the odometric modulus of compressibility is in the range of 45.1 to 116.7 depending on the loading conditions) and tests for triple axial compression (two samples, both with a diameter of 3.8 cm and a height of 7.6 cm; the destroying pressure was found to be equal to 0.5 and 0.27 MPa).}
journal = []
volume = {339}
journal type = {AC}
place = {Poland}
year = {1980}
month = {Jan}
}
title = {Study of the mechanical properties of brown coal}
author = {Okruszek, Z}
abstractNote = {The techniques and the results of studies of the mechanical properties of brown coal discovered in a zone adjacent to the location of the Rogowiec power plant (Poland) are described. The studies were conducted by the geotechnical laboratory of the Polytechnical Institute in the city of Lodz. Included in the program of studies were: tests of the brown coal (eight samples with a diameter to height ratio of d/h = 10.0/7.5; 11.1/7.8; 9.3/8.8; 8.1/6.8; 8.5/9.4; 8.0/8.8; 7.9/7.6 adn 8.8/8.6; dimensions in centimeters) for single axis compression (destroying stress was found to be 0.778; 0.660; 0.376; 0.804; 0.140; 0.472; 0.408 and 0.278 MPa); tests of samples (five units) for shear strength (the chip force is 0.36; 0.46; 0.39; 0.11 and 0.36 kilonewtons); tests of the samples (two samples, both with a diameter of 3.8 cm and a height of 7.6 cm) for stretching (the destructive force is 50.1 and 54.9 kilonewtons); odometric tests to determine the odometric modulus of compressibility of the brown coal (a total of four samples; three of which were loaded by a force in the range of 0.6-1.2 MPa and one in the range of 0-1.1 MPa; the odometric modulus of compressibility is in the range of 45.1 to 116.7 depending on the loading conditions) and tests for triple axial compression (two samples, both with a diameter of 3.8 cm and a height of 7.6 cm; the destroying pressure was found to be equal to 0.5 and 0.27 MPa).}
journal = []
volume = {339}
journal type = {AC}
place = {Poland}
year = {1980}
month = {Jan}
}