Abstract
The preparation of a cellulose derivative containing salicylic acid as functional group was varied in order to find optimal conditions with respect to fast exchange as well as high capacity. Two kinds of cellulose (cross-linked and microcrystalline) and different reaction times were used. The properties of the products were investigated by titration curves to determine the capacity and by measuring the non-isotopic exchange Na/sup +//*Fe/sup 3 +/ and the isotopic exchange *Fe/sup 3 +//Fe/sup 3 +/ as a function of time. Microcrystalline cellulose and a reaction time of 15 min gave optimal results.
Lieser, K H;
Foerster, M;
Burba, P
[1]
- Technische Hochschule Darmstadt (Germany, F.R.). Fachbereich Anorganische Chemie und Kernchemie
Citation Formats
Lieser, K H, Foerster, M, and Burba, P.
Effect of the conditions of preparation on the properties of a cellulose exchanger containing salicylic acid as a functional group.
Germany: N. p.,
1977.
Web.
Lieser, K H, Foerster, M, & Burba, P.
Effect of the conditions of preparation on the properties of a cellulose exchanger containing salicylic acid as a functional group.
Germany.
Lieser, K H, Foerster, M, and Burba, P.
1977.
"Effect of the conditions of preparation on the properties of a cellulose exchanger containing salicylic acid as a functional group."
Germany.
@misc{etde_5439589,
title = {Effect of the conditions of preparation on the properties of a cellulose exchanger containing salicylic acid as a functional group}
author = {Lieser, K H, Foerster, M, and Burba, P}
abstractNote = {The preparation of a cellulose derivative containing salicylic acid as functional group was varied in order to find optimal conditions with respect to fast exchange as well as high capacity. Two kinds of cellulose (cross-linked and microcrystalline) and different reaction times were used. The properties of the products were investigated by titration curves to determine the capacity and by measuring the non-isotopic exchange Na/sup +//*Fe/sup 3 +/ and the isotopic exchange *Fe/sup 3 +//Fe/sup 3 +/ as a function of time. Microcrystalline cellulose and a reaction time of 15 min gave optimal results.}
journal = []
volume = {284:3}
journal type = {AC}
place = {Germany}
year = {1977}
month = {Apr}
}
title = {Effect of the conditions of preparation on the properties of a cellulose exchanger containing salicylic acid as a functional group}
author = {Lieser, K H, Foerster, M, and Burba, P}
abstractNote = {The preparation of a cellulose derivative containing salicylic acid as functional group was varied in order to find optimal conditions with respect to fast exchange as well as high capacity. Two kinds of cellulose (cross-linked and microcrystalline) and different reaction times were used. The properties of the products were investigated by titration curves to determine the capacity and by measuring the non-isotopic exchange Na/sup +//*Fe/sup 3 +/ and the isotopic exchange *Fe/sup 3 +//Fe/sup 3 +/ as a function of time. Microcrystalline cellulose and a reaction time of 15 min gave optimal results.}
journal = []
volume = {284:3}
journal type = {AC}
place = {Germany}
year = {1977}
month = {Apr}
}