Abstract
In this study some alternative catalysts for oxygen reduction in an alkaline electrolyte (7 M KOH) were tested. The catalysts tested were: CoTMPP, LaNiO{sub 3}, Pt (for comparison) and MnO{sub 2}. The electrodes were manufactured by the rolling method. The best electrodes made in this way has been tested in a long run test, testing times ranging from 425 hours to 660 hours. The decay in potential during the 660 hour run was 0.041 mV/h.
Lamminen, J;
Lampinen, M J;
Viitanen, M;
Vuorisalo, J;
[1]
Kivisaari, J
[2]
- Helsinki Univ. of Technology, Otaniemi (Finland). Lab. of Thermal Engineering
- The Royal Inst. of Technology, Stockholm (Sweden). Dept. of Chemical Technology
Citation Formats
Lamminen, J, Lampinen, M J, Viitanen, M, Vuorisalo, J, and Kivisaari, J.
Manufacture of air electrodes and long run tests.
Finland: N. p.,
1990.
Web.
Lamminen, J, Lampinen, M J, Viitanen, M, Vuorisalo, J, & Kivisaari, J.
Manufacture of air electrodes and long run tests.
Finland.
Lamminen, J, Lampinen, M J, Viitanen, M, Vuorisalo, J, and Kivisaari, J.
1990.
"Manufacture of air electrodes and long run tests."
Finland.
@misc{etde_10110746,
title = {Manufacture of air electrodes and long run tests}
author = {Lamminen, J, Lampinen, M J, Viitanen, M, Vuorisalo, J, and Kivisaari, J}
abstractNote = {In this study some alternative catalysts for oxygen reduction in an alkaline electrolyte (7 M KOH) were tested. The catalysts tested were: CoTMPP, LaNiO{sub 3}, Pt (for comparison) and MnO{sub 2}. The electrodes were manufactured by the rolling method. The best electrodes made in this way has been tested in a long run test, testing times ranging from 425 hours to 660 hours. The decay in potential during the 660 hour run was 0.041 mV/h.}
place = {Finland}
year = {1990}
month = {Dec}
}
title = {Manufacture of air electrodes and long run tests}
author = {Lamminen, J, Lampinen, M J, Viitanen, M, Vuorisalo, J, and Kivisaari, J}
abstractNote = {In this study some alternative catalysts for oxygen reduction in an alkaline electrolyte (7 M KOH) were tested. The catalysts tested were: CoTMPP, LaNiO{sub 3}, Pt (for comparison) and MnO{sub 2}. The electrodes were manufactured by the rolling method. The best electrodes made in this way has been tested in a long run test, testing times ranging from 425 hours to 660 hours. The decay in potential during the 660 hour run was 0.041 mV/h.}
place = {Finland}
year = {1990}
month = {Dec}
}