<?xml version="1.0" encoding="UTF-8" ?>
<rdf:RDF xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:dcq="http://purl.org/dc/terms/" xmlns:rdf="http://www.w3.org/1999/02/22-rdf-syntax-ns#">
     <records>
	  <record>
	       <dc:title>Electrochemical properties of nickel-precipitated pyrite as cathode active material for lithium/pyrite cell</dc:title>
	       <dc:creator>Choi, Y J; Kim, N W [i-Cube Center, ITRC for Energy Storage and Conversion, Gyeongsang National University, 900 Gazwadong, Jinju, Gyeongnam 660-701 (Korea, Republic of)]; Kim, K.W., E-mail: kiwonkim@gnu.ac.k [i-Cube Center, ITRC for Energy Storage and Conversion, Gyeongsang National University, 900 Gazwadong, Jinju, Gyeongnam 660-701 (Korea, Republic of)]; Cho, K K; Cho, G B; Ahn, H J; Ahn, J H [i-Cube Center, ITRC for Energy Storage and Conversion, Gyeongsang National University, 900 Gazwadong, Jinju, Gyeongnam 660-701 (Korea, Republic of)]; Ryu, K S [Department of Chemistry, University of Ulsan, Ulsan 680-749 (Korea, Republic of)]; Gu, H B [Department of Electrical Engineering, College of Engineering, Chonnam National University, 300 Yongbong-dong, Buk-ku, Kwangju (Korea, Republic of)]</dc:creator>
	       <dc:subject>36 MATERIALS SCIENCE; CATHODES; EFFICIENCY; ELECTROCHEMICAL CELLS; ELECTROCHEMISTRY; LITHIUM; NICKEL; OXIDATION; PLATING; PRECIPITATION; PYRITE; ALKALI METALS; CHEMICAL REACTIONS; CHEMISTRY; DEPOSITION; ELECTRODES; ELEMENTS; METALS; MINERALS; SEPARATION PROCESSES; SULFIDE MINERALS; SURFACE COATING; TRANSITION ELEMENTS</dc:subject>
	       <dc:subjectRelated>ALKALI METALS; CHEMICAL REACTIONS; CHEMISTRY; DEPOSITION; ELECTRODES; ELEMENTS; METALS; MINERALS; SEPARATION PROCESSES; SULFIDE MINERALS; SURFACE COATING; TRANSITION ELEMENTS</dc:subjectRelated>
	       <dc:description>The effects of nickel precipitation and the cut-off voltage on the electrochemical properties of a pyrite cathode were investigated by using an electroless nickel-plating method. After nickel precipitation, some nickel particles that were precipitated on the surface of pyrite accumulated between the pyrite powder particles. In the voltage range of 0.4-3.2 V, a cell with nickel-precipitated pyrite exhibited a rapid decrease in discharge capacity and poor columbic efficiency. On the other hand, in the voltage range of 0.8-2.4 V, the cell showed an improved cycle life property and good coulombic efficiency because irreversible reactions below 0.8 V and sulfur oxidation above 2.4 V were suppressed by controlling the cut-off potential and the internal resistance was decreased by nickel precipitation.</dc:description>
	       <dcq:publisher></dcq:publisher>
	       <dcq:publisherResearch></dcq:publisherResearch>
	       <dcq:publisherAvailability>Available from http://dx.doi.org/10.1016/j.jallcom.2009.05.140</dcq:publisherAvailability>
	       <dcq:publisherSponsor></dcq:publisherSponsor>
	       <dcq:publisherCountry>Netherlands</dcq:publisherCountry>
		   <dc:contributingOrganizations></dc:contributingOrganizations>
	       <dc:date>2009-10-19</dc:date>
	       <dc:language>English</dc:language>
	       <dc:type>Journal Article</dc:type>
	       <dcq:typeQualifier></dcq:typeQualifier>
	       <dc:relation>Journal Name: Journal of Alloys and Compounds; Journal Volume: 485; Journal Issue: 1-2; Other Information: DOI: 10.1016/j.jallcom.2009.05.140; PII: S0925-8388(09)01133-5; Copyright (c) 2009 Elsevier Science B.V., Amsterdam, The Netherlands, All rights reserved.</dc:relation>
	       <dc:coverage></dc:coverage>
	       <dc:format>Medium: X; Size: page(s) 462-466</dc:format>
	       <dc:doi>https://doi.org/10.1016/j.jallcom.2009.05.140</dc:doi>
	       <dc:identifier></dc:identifier>
		   <dc:journalName>[]</dc:journalName>
		   <dc:journalIssue>1-2</dc:journalIssue>
		   <dc:journalVolume>485</dc:journalVolume>
	       <dc:identifierReport></dc:identifierReport>
	       <dcq:identifierDOEcontract></dcq:identifierDOEcontract>
	       <dc:identifierOther>Journal ID: ISSN 0925-8388; JALCEU; TRN: NL10R1351119524</dc:identifierOther>
	       <dc:source>NLN</dc:source>
	       <dc:rights></dc:rights>
	       <dc:dateEntry>2012-12-21</dc:dateEntry>
	       <dc:dateAdded></dc:dateAdded>
	       <dc:ostiId>21392101</dc:ostiId>
	       <dcq:identifier-purl></dcq:identifier-purl>
	  </record>
     </records>
</rdf:RDF>