Abstract

New polymer compositions based on poly(2,6-dimethyl-1,4-phenylene oxide) and other high-softening-temperature polymers are disclosed. These materials have a microphase domain structure that has an ionically-conductive phase and a phase with good mechanical strength and a high softening temperature. In one arrangement, the structural block has a softening temperature of about 210.degree. C. These materials can be made with either homopolymers or with block copolymers.

Inventors:
; ;
Issue Date:
Research Org.:
Seeo, Inc., Hayward, CA (United States)
Sponsoring Org.:
USDOE
OSTI Identifier:
1215545
Patent Number(s):
9133338
Application Number:
13/698,664
Assignee:
Seeo, Inc. (Hayward, CA)
Patent Classifications (CPCs):
C - CHEMISTRY C08 - ORGANIC MACROMOLECULAR COMPOUNDS C08G - MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
C - CHEMISTRY C08 - ORGANIC MACROMOLECULAR COMPOUNDS C08L - COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
DOE Contract Number:  
OE0000223
Resource Type:
Patent
Resource Relation:
Patent File Date: 2011 May 19
Country of Publication:
United States
Language:
English
Subject:
36 MATERIALS SCIENCE

Citation Formats

Yang, Jin, Eitouni, Hany Basam, and Singh, Mohit. Polymer compositions based on PXE. United States: N. p., 2015. Web.
Yang, Jin, Eitouni, Hany Basam, & Singh, Mohit. Polymer compositions based on PXE. United States.
Yang, Jin, Eitouni, Hany Basam, and Singh, Mohit. Tue . "Polymer compositions based on PXE". United States. https://www.osti.gov/servlets/purl/1215545.
@article{osti_1215545,
title = {Polymer compositions based on PXE},
author = {Yang, Jin and Eitouni, Hany Basam and Singh, Mohit},
abstractNote = {New polymer compositions based on poly(2,6-dimethyl-1,4-phenylene oxide) and other high-softening-temperature polymers are disclosed. These materials have a microphase domain structure that has an ionically-conductive phase and a phase with good mechanical strength and a high softening temperature. In one arrangement, the structural block has a softening temperature of about 210.degree. C. These materials can be made with either homopolymers or with block copolymers.},
doi = {},
journal = {},
number = ,
volume = ,
place = {United States},
year = {Tue Sep 15 00:00:00 EDT 2015},
month = {Tue Sep 15 00:00:00 EDT 2015}
}

Works referenced in this record:

Organic electrolyte battery
patent, August 2001


Solid polymer electrolytes
patent, November 2003


Solid polymer electrolyte
patent-application, November 2005


Solid Electrolyte Material Manufacturable by Polymer Processing Methods
patent-application, March 2009


Anionic polymerization of oxirane in the presence of the polyiminophosphazene base t-Bu-P4
journal, February 1996


Synthesis of α,ω-Heterobifunctional Poly(ethylene glycol)s by Metal-Free Anionic Ring-Opening Polymerization
journal, May 2001


Polyisobutylene-block-Poly(ethylene oxide) for Robust Templating of Highly Ordered Mesoporous Materials
journal, April 2005


ATRP of Amphiphilic Graft Copolymers Based on PVDF and Their Use as Membrane Additives
journal, September 2002


    Works referencing / citing this record:

    Polymer compositions based on PXE
    patent, September 2015