Title: Method of forming a hardened surface on a substrate

Abstract

The invention includes a method of producing a hard metallic material by forming a mixture containing at least 55% iron and at least one of B, C, Si and P. The mixture is formed into an alloy and cooled to form a metallic material having a hardness of greater than about 9.2 GPa. The invention includes a method of forming a wire by combining a metal strip and a powder. The metal strip and the powder are rolled to form a wire containing at least 55% iron and from two to seven additional elements including at least one of C, Si and B. The invention also includes a method of forming a hardened surface on a substrate by processing a solid mass to form a powder, applying the powder to a surface to form a layer containing metallic glass, and converting the glass to a crystalline material having a nanocrystalline grain size.

Inventors:
 [1]
  1. Iona, ID
Issue Date:
Research Org.:
Idaho National Laboratory (INL), Idaho Falls, ID (United States)
Sponsoring Org.:
USDOE
OSTI Identifier:
1013610
Patent Number(s):
7785428
Application Number:
10/753,167
Assignee:
Battelle Energy Alliance, LLC (Idaho Falls, ID)
Patent Classifications (CPCs):
B - PERFORMING OPERATIONS B22 - CASTING B22F - WORKING METALLIC POWDER
B - PERFORMING OPERATIONS B23 - MACHINE TOOLS B23K - SOLDERING OR UNSOLDERING
DOE Contract Number:  
AC07-99ID13727
Resource Type:
Patent
Country of Publication:
United States
Language:
English

Citation Formats

Branagan, Daniel J. Method of forming a hardened surface on a substrate. United States: N. p., 2010. Web.
Branagan, Daniel J. Method of forming a hardened surface on a substrate. United States.
Branagan, Daniel J. Tue . "Method of forming a hardened surface on a substrate". United States. https://www.osti.gov/servlets/purl/1013610.
@article{osti_1013610,
title = {Method of forming a hardened surface on a substrate},
author = {Branagan, Daniel J},
abstractNote = {The invention includes a method of producing a hard metallic material by forming a mixture containing at least 55% iron and at least one of B, C, Si and P. The mixture is formed into an alloy and cooled to form a metallic material having a hardness of greater than about 9.2 GPa. The invention includes a method of forming a wire by combining a metal strip and a powder. The metal strip and the powder are rolled to form a wire containing at least 55% iron and from two to seven additional elements including at least one of C, Si and B. The invention also includes a method of forming a hardened surface on a substrate by processing a solid mass to form a powder, applying the powder to a surface to form a layer containing metallic glass, and converting the glass to a crystalline material having a nanocrystalline grain size.},
doi = {},
journal = {},
number = ,
volume = ,
place = {United States},
year = {Tue Aug 31 00:00:00 EDT 2010},
month = {Tue Aug 31 00:00:00 EDT 2010}
}