Title: Method of making a composite refractory material

Abstract

A composite refractory material is prepared by combining boron carbide with furan resin to form a mixture containing about 8 wt. % furan resin. The mixture is formed into a pellet which is placed into a grit pack comprising an oxide of an element such as yttrium to form a sinterable body. The sinterable body is sintered under vacuum with microwave energy at a temperature no greater than 2000.degree. C. to form a composite refractory material.

Inventors:
 [1];  [2]
  1. Kingston, TN
  2. Knoxville, TN
Issue Date:
Research Org.:
Oak Ridge National Laboratory (ORNL), Oak Ridge, TN (United States)
OSTI Identifier:
870078
Patent Number(s):
5453225
Assignee:
Martin Marietta Energy Systems, Inc. (Oak Ridge, TN)
Patent Classifications (CPCs):
C - CHEMISTRY C04 - CEMENTS C04B - LIME, MAGNESIA
DOE Contract Number:  
AC05-84OR21400
Resource Type:
Patent
Country of Publication:
United States
Language:
English
Subject:
method; composite; refractory; material; prepared; combining; boron; carbide; furan; resin; form; mixture; containing; wt; formed; pellet; placed; grit; pack; comprising; oxide; element; yttrium; sinterable; sintered; vacuum; microwave; energy; temperature; 2000; degree; boron carbide; refractory material; mixture containing; microwave energy; wave energy; composite refractory; furan resin; /264/

Citation Formats

Morrow, Marvin S, and Holcombe, Cressie E. Method of making a composite refractory material. United States: N. p., 1995. Web.
Morrow, Marvin S, & Holcombe, Cressie E. Method of making a composite refractory material. United States.
Morrow, Marvin S, and Holcombe, Cressie E. Sun . "Method of making a composite refractory material". United States. https://www.osti.gov/servlets/purl/870078.
@article{osti_870078,
title = {Method of making a composite refractory material},
author = {Morrow, Marvin S and Holcombe, Cressie E},
abstractNote = {A composite refractory material is prepared by combining boron carbide with furan resin to form a mixture containing about 8 wt. % furan resin. The mixture is formed into a pellet which is placed into a grit pack comprising an oxide of an element such as yttrium to form a sinterable body. The sinterable body is sintered under vacuum with microwave energy at a temperature no greater than 2000.degree. C. to form a composite refractory material.},
doi = {},
journal = {},
number = ,
volume = ,
place = {United States},
year = {Sun Jan 01 00:00:00 EST 1995},
month = {Sun Jan 01 00:00:00 EST 1995}
}