This work describes a high strength, high toughness bainitic/ferritic steel alloy comprising about 2.75% to 4.0% chromium, about 2.0% to 3.5% tungsten, about 0.10% to 0.30% vanadium, and about 0.1% to 0.15% carbon with the balance iron, wherein the percentages are by total weight of the composition, wherein the alloy having been heated to an austenitizing temperature and then cooled at a rate sufficient to produce carbide-free acicular bainite. 15 figures.
- Inventors:
- Issue Date:
- OSTI Identifier:
- 7275722
- Patent Number(s):
- 5292384
- Application Number:
- PPN: US 7-914452
- Assignee:
- Martin Marietta Energy Systems, Inc., Oak Ridge, TN (United States)
- DOE Contract Number:
- AC05-84OR21400
- Resource Type:
- Patent
- Resource Relation:
- Patent File Date: 17 Jul 1992
- Country of Publication:
- United States
- Language:
- English
- Subject:
- 36 MATERIALS SCIENCE; 70 PLASMA PHYSICS AND FUSION TECHNOLOGY; Ma; FERRITIC STEELS; FABRICATION; MECHANICAL PROPERTIES; BAINITE; CHEMICAL COMPOSITION; RADIOACTIVITY; THERMONUCLEAR REACTOR MATERIALS; ALLOYS; IRON ALLOYS; IRON BASE ALLOYS; MATERIALS; STEELS; 360101* - Metals & Alloys- Preparation & Fabrication; 360103 - Metals & Alloys- Mechanical Properties; 700480 - Fusion Technology- Component Development; Materials Studies- (1992-)
Citation Formats
Klueh, R L, and Maziasz, P J. Cr-W-V bainitic/ferritic steel with improved strength and toughness and method of making. United States: N. p., 1994.
Web.
Klueh, R L, & Maziasz, P J. Cr-W-V bainitic/ferritic steel with improved strength and toughness and method of making. United States.
Klueh, R L, and Maziasz, P J. Tue .
"Cr-W-V bainitic/ferritic steel with improved strength and toughness and method of making". United States.
@article{osti_7275722,
title = {Cr-W-V bainitic/ferritic steel with improved strength and toughness and method of making},
author = {Klueh, R L and Maziasz, P J},
abstractNote = {This work describes a high strength, high toughness bainitic/ferritic steel alloy comprising about 2.75% to 4.0% chromium, about 2.0% to 3.5% tungsten, about 0.10% to 0.30% vanadium, and about 0.1% to 0.15% carbon with the balance iron, wherein the percentages are by total weight of the composition, wherein the alloy having been heated to an austenitizing temperature and then cooled at a rate sufficient to produce carbide-free acicular bainite. 15 figures.},
doi = {},
journal = {},
number = ,
volume = ,
place = {United States},
year = {1994},
month = {3}
}