Title: Filler metal alloy for welding cast nickel aluminide alloys

Abstract

A filler metal alloy used as a filler for welding cast nickel aluminide alloys contains from about 15 to about 17 wt. % chromium, from about 4 to about 5 wt. % aluminum, equal to or less than about 1.5 wt. % molybdenum, from about 1 to about 4.5 wt. % zirconium, equal to or less than about 0.01 wt. % yttrium, equal to or less than about 0.01 wt. % boron and the balance nickel. The filler metal alloy is made by melting and casting techniques such as are melting the components of the filler metal alloy and cast in copper chill molds. 3 figs.

Inventors:
;
Issue Date:
Research Org.:
Oak Ridge National Laboratory (ORNL), Oak Ridge, TN (United States)
Sponsoring Org.:
USDOE, Washington, DC (United States)
OSTI Identifier:
597158
Patent Number(s):
5725693
Application Number:
PAN: 8-611,863
Assignee:
Lockheed Martin Energy Systems, Inc., Oak Ridge, TN (United States)
DOE Contract Number:  
AC05-84OR21400
Resource Type:
Patent
Resource Relation:
Other Information: PBD: 10 Mar 1998
Country of Publication:
United States
Language:
English
Subject:
36 MATERIALS SCIENCE; FILLER METALS; NICKEL BASE ALLOYS; WELDING; ALUMINIUM ALLOYS; CHROMIUM ALLOYS; YTTRIUM ADDITIONS; MOLYBDENUM ALLOYS; ZIRCONIUM ALLOYS; BORON ADDITIONS

Citation Formats

Santella, M L, and Sikka, V K. Filler metal alloy for welding cast nickel aluminide alloys. United States: N. p., 1998. Web.
Santella, M L, & Sikka, V K. Filler metal alloy for welding cast nickel aluminide alloys. United States.
Santella, M L, and Sikka, V K. Tue . "Filler metal alloy for welding cast nickel aluminide alloys". United States.
@article{osti_597158,
title = {Filler metal alloy for welding cast nickel aluminide alloys},
author = {Santella, M L and Sikka, V K},
abstractNote = {A filler metal alloy used as a filler for welding cast nickel aluminide alloys contains from about 15 to about 17 wt. % chromium, from about 4 to about 5 wt. % aluminum, equal to or less than about 1.5 wt. % molybdenum, from about 1 to about 4.5 wt. % zirconium, equal to or less than about 0.01 wt. % yttrium, equal to or less than about 0.01 wt. % boron and the balance nickel. The filler metal alloy is made by melting and casting techniques such as are melting the components of the filler metal alloy and cast in copper chill molds. 3 figs.},
doi = {},
journal = {},
number = ,
volume = ,
place = {United States},
year = {1998},
month = {3}
}

Patent:
Search for the full text at the U.S. Patent and Trademark Office Note: You will be redirected to the USPTO site, which may require a pop-up blocker to be deactivated to view the patent. If so, you will need to manually turn off your browser's pop-up blocker, typically found within the browser settings. (See DOE Patents FAQs for more information.)