Title: METHOD OF MAKING DELTA ZIRCONIUM HYDRIDE MONOLITHIC MODERATOR PIECES

Abstract

A method is given for preparing large, sound bodies of delta zirconium hydride. The method includes the steps of heating a zirconium body to a temperature of not less than l000 deg C, providing a hydrogen atmosphere for the zirconium body at a pressure not greater than one atmosphere, reducing the temperature slowly to 800 deg C at such a rate that cracks do not form while maintaining the hydrogen pressure substantially constant, and cooling in an atmosphere of hydrogen. (AEC)

Inventors:
Issue Date:
OSTI Identifier:
4819136
Patent Number(s):
3018169
Assignee:
U.S. Atomic Energy Commission
Patent Classifications (CPCs):
Y - NEW / CROSS SECTIONAL TECHNOLOGIES Y02 - TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE Y02E - REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
G - PHYSICS G21 - NUCLEAR PHYSICS G21C - NUCLEAR REACTORS
NSA Number:
NSA-16-004524
Resource Type:
Patent
Resource Relation:
Other Information: Orig. Receipt Date: 31-DEC-62
Country of Publication:
United States
Language:
English
Subject:
METALS, CERAMICS, AND OTHER MATERIALS; ALLOTROPY; COOLING; CRACKS; FABRICATION; HEATING; HIGH TEMPERATURE; HYDROGEN; MODERATORS; PREPARATION; PRESSURE; ZIRCONIUM HYDRIDES

Citation Formats

Vetrano, J B. METHOD OF MAKING DELTA ZIRCONIUM HYDRIDE MONOLITHIC MODERATOR PIECES. United States: N. p., 1962. Web.
Vetrano, J B. METHOD OF MAKING DELTA ZIRCONIUM HYDRIDE MONOLITHIC MODERATOR PIECES. United States.
Vetrano, J B. Tue . "METHOD OF MAKING DELTA ZIRCONIUM HYDRIDE MONOLITHIC MODERATOR PIECES". United States.
@article{osti_4819136,
title = {METHOD OF MAKING DELTA ZIRCONIUM HYDRIDE MONOLITHIC MODERATOR PIECES},
author = {Vetrano, J B},
abstractNote = {A method is given for preparing large, sound bodies of delta zirconium hydride. The method includes the steps of heating a zirconium body to a temperature of not less than l000 deg C, providing a hydrogen atmosphere for the zirconium body at a pressure not greater than one atmosphere, reducing the temperature slowly to 800 deg C at such a rate that cracks do not form while maintaining the hydrogen pressure substantially constant, and cooling in an atmosphere of hydrogen. (AEC)},
doi = {},
journal = {},
number = ,
volume = ,
place = {United States},
year = {1962},
month = {1}
}