Title: METHOD FOR OBTAINING PLUTONIUM METAL FROM ITS TRICHLORIDE

Abstract

A method was developed for obtaining plutonium metal by direct reduction of plutonium chloride, without the use of a booster, using calcium and lanthamum as a reductant, the said reduction being carried out at temperature in the range of 700 to 850 deg C and at about atmospheric pressure. (AEC)

Inventors:
; ;
Issue Date:
Research Org.:
Originating Research Org. not identified
OSTI Identifier:
4812501
Patent Number(s):
3049423
Assignee:
U.S. Atomic Energy Commission DTIE; NSA-16-025711
NSA Number:
NSA-16-025711
Resource Type:
Patent
Resource Relation:
Other Information: Orig. Receipt Date: 31-DEC-62
Country of Publication:
United States
Language:
English
Subject:
METALS, CERAMICS, AND OTHER MATERIALS; CALCIUM; HIGH TEMPERATURE; LANTHANUM; PLUTONIUM; PLUTONIUM CHLORIDES; PREPARATION; REDUCTION

Citation Formats

Reavis, J.G., Leary, J.A., and Maraman, W.J. METHOD FOR OBTAINING PLUTONIUM METAL FROM ITS TRICHLORIDE. United States: N. p., 1962. Web.
Reavis, J.G., Leary, J.A., & Maraman, W.J. METHOD FOR OBTAINING PLUTONIUM METAL FROM ITS TRICHLORIDE. United States.
Reavis, J.G., Leary, J.A., and Maraman, W.J. Tue . "METHOD FOR OBTAINING PLUTONIUM METAL FROM ITS TRICHLORIDE". United States.
@article{osti_4812501,
title = {METHOD FOR OBTAINING PLUTONIUM METAL FROM ITS TRICHLORIDE},
author = {Reavis, J.G. and Leary, J.A. and Maraman, W.J.},
abstractNote = {A method was developed for obtaining plutonium metal by direct reduction of plutonium chloride, without the use of a booster, using calcium and lanthamum as a reductant, the said reduction being carried out at temperature in the range of 700 to 850 deg C and at about atmospheric pressure. (AEC)},
doi = {},
journal = {},
number = ,
volume = ,
place = {United States},
year = {1962},
month = {8}
}