Title: DIMENSION STABILIZED FIXED PHOTOGRAPHIC TYPE EMULSION AND A METHOD FOR PRODUCING SAME

Abstract

A process is given for stabilizing the dimensions of fixed gelatin-base photographic type emulsions containing silver halide, and particularly to such emulsions containing large amounts of silver chloride for use as nuclear track emulsions, so that the dimensions of the final product are the same as or in a predetermined fixed ratio to the dimensions of the emulsions prior to exposure. The process comprises contacting an exposed, fixed emulsion with a solution of wood rosin dissolved in ethyl alcohol for times corresponding to the dimensions desired, and thereafter permitting the alcohol to evaporate. (AEC)

Inventors:
Issue Date:
Research Org.:
Originating Research Org. not identified
OSTI Identifier:
4793059
Patent Number(s):
3025162
Assignee:
U.S. Atomic Energy Commission DTIE; NSA-16-010260
NSA Number:
NSA-16-010260
Resource Type:
Patent
Resource Relation:
Other Information: Orig. Receipt Date: 31-DEC-62
Country of Publication:
United States
Language:
English
Subject:
ENGINEERING AND EQUIPMENT; ALCOHOLS; COLLOIDS; ETHANOL; EVAPORATION; HALIDES; NUCLEAR EMULSIONS; PARTICLE TRACKS; PHOTOGRAPHIC FILM; SILVER CHLORIDES; SILVER COMPOUNDS; STABILITY

Citation Formats

Gilbert, F.C. DIMENSION STABILIZED FIXED PHOTOGRAPHIC TYPE EMULSION AND A METHOD FOR PRODUCING SAME. United States: N. p., 1962. Web.
Gilbert, F.C. DIMENSION STABILIZED FIXED PHOTOGRAPHIC TYPE EMULSION AND A METHOD FOR PRODUCING SAME. United States.
Gilbert, F.C. Tue . "DIMENSION STABILIZED FIXED PHOTOGRAPHIC TYPE EMULSION AND A METHOD FOR PRODUCING SAME". United States.
@article{osti_4793059,
title = {DIMENSION STABILIZED FIXED PHOTOGRAPHIC TYPE EMULSION AND A METHOD FOR PRODUCING SAME},
author = {Gilbert, F.C.},
abstractNote = {A process is given for stabilizing the dimensions of fixed gelatin-base photographic type emulsions containing silver halide, and particularly to such emulsions containing large amounts of silver chloride for use as nuclear track emulsions, so that the dimensions of the final product are the same as or in a predetermined fixed ratio to the dimensions of the emulsions prior to exposure. The process comprises contacting an exposed, fixed emulsion with a solution of wood rosin dissolved in ethyl alcohol for times corresponding to the dimensions desired, and thereafter permitting the alcohol to evaporate. (AEC)},
doi = {},
journal = {},
number = ,
volume = ,
place = {United States},
year = {1962},
month = {3}
}