Title: METHOD OF PREPARING METAL HALIDES

Abstract

The conversion of plutonium halides from plutonium peroxide can be done by washing the peroxide with hydrogen peroxide, drying the peroxide, passing a dry gaseous hydrohalide over the surface of the peroxide at a temperature of about lOO icient laborato C until the reaction rate has stabillzed, and then ralsing the reaction temperature to between 400 and 600 icient laborato C until the conversion to plutonium halide is substantially complete.

Inventors:
Issue Date:
Research Org.:
Originating Research Org. not identified
OSTI Identifier:
4296277
Patent Number(s):
2860950
Assignee:
U.S. Atomic Energy Commission
Patent Classifications (CPCs):
C - CHEMISTRY C01 - INORGANIC CHEMISTRY C01G - COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F
NSA Number:
NSA-13-008404
Resource Type:
Patent
Resource Relation:
Other Information: Orig. Receipt Date: 31-DEC-59
Country of Publication:
United States
Language:
English
Subject:
PATENTS; CHEMICAL REACTIONS; CONVERSION; EVAPORATION; GASES; HALIDES; HALOGENS; HIGH TEMPERATURE; HYDROBROMIC ACID; HYDROCHLORIC ACID; HYDROFLUORIC ACID; HYDROGEN PEROXIDES; METALS; OXIDES; PEROXIDES; PLUTONIUM COMPOUNDS; PLUTONIUM OXIDES; PREPARATION; REACTION KINETICS; SURFACES; TEMPERATURE

Citation Formats

Hendrickson, A V. METHOD OF PREPARING METAL HALIDES. United States: N. p., 1958. Web.
Hendrickson, A V. METHOD OF PREPARING METAL HALIDES. United States.
Hendrickson, A V. Tue . "METHOD OF PREPARING METAL HALIDES". United States.
@article{osti_4296277,
title = {METHOD OF PREPARING METAL HALIDES},
author = {Hendrickson, A V},
abstractNote = {The conversion of plutonium halides from plutonium peroxide can be done by washing the peroxide with hydrogen peroxide, drying the peroxide, passing a dry gaseous hydrohalide over the surface of the peroxide at a temperature of about lOO icient laborato C until the reaction rate has stabillzed, and then ralsing the reaction temperature to between 400 and 600 icient laborato C until the conversion to plutonium halide is substantially complete.},
doi = {},
journal = {},
number = ,
volume = ,
place = {United States},
year = {1958},
month = {11}
}

Patent:
Search for the full text at the U.S. Patent and Trademark Office Note: You will be redirected to the USPTO site, which may require a pop-up blocker to be deactivated to view the patent. If so, you will need to manually turn off your browser's pop-up blocker, typically found within the browser settings. (See DOE Patents FAQs for more information.)

Save / Share: