Title: METHOD OF HEAT-TREATING URANIUM-SILICON ALLOYS

Abstract

A process is presented for manufacturing uranium alloys of a high degree of dimensional stability and free from thermal expansion. The process involves incorporating 0.01 to 0.1% by weight silicon into uranium, rolling the alloy obtained at a temperature below 660 deg C, beta-heating the alloy to a temperature of between 660 and 770 deg C and quenching the alloy.

Inventors:
Issue Date:
Research Org.:
Originating Research Org. not identified
OSTI Identifier:
4234334
Patent Number(s):
2898252
Assignee:
U.S. Atomic Energy Commission DTIE; NSA-14-002715
NSA Number:
NSA-14-002715
Resource Type:
Patent
Resource Relation:
Other Information: Orig. Receipt Date: 31-DEC-60
Country of Publication:
United States
Language:
English
Subject:
METALS, CERAMICS, AND MATERIALS; EXPANSION; FABRICATION; HEAT TREATMENTS; HIGH TEMPERATURE; QUENCHING; ROLLING; SILICIDES; SILICON; STABILITY; TEMPERATURE; URANIUM; URANIUM ALLOYS

Citation Formats

Zegler, S.T. METHOD OF HEAT-TREATING URANIUM-SILICON ALLOYS. United States: N. p., 1959. Web.
Zegler, S.T. METHOD OF HEAT-TREATING URANIUM-SILICON ALLOYS. United States.
Zegler, S.T. Sat . "METHOD OF HEAT-TREATING URANIUM-SILICON ALLOYS". United States.
@article{osti_4234334,
title = {METHOD OF HEAT-TREATING URANIUM-SILICON ALLOYS},
author = {Zegler, S.T.},
abstractNote = {A process is presented for manufacturing uranium alloys of a high degree of dimensional stability and free from thermal expansion. The process involves incorporating 0.01 to 0.1% by weight silicon into uranium, rolling the alloy obtained at a temperature below 660 deg C, beta-heating the alloy to a temperature of between 660 and 770 deg C and quenching the alloy.},
doi = {},
journal = {},
number = ,
volume = ,
place = {United States},
year = {1959},
month = {8}
}