Title: METHOD OF REDUCING PLUTONIUM WITH FERROUS IONS

Abstract

A process is presented for separating hexavalent plutonium from fission product values. To a nitric acid solution containing the values, ferrous ions are added and the solution is heated and held at elevated temperature to convert the plutonium to the tetravalent state via the trivalent state and the plutonium is then selectively precipitated on a BiPO/sub 4/ or LaF/sub 3/ carrier. The tetravalent plutonium formed is optionally complexed with fluoride, oxalate, or phosphate anion prior to carrier precipitation.

Inventors:
; ; ;
Issue Date:
Research Org.:
Originating Research Org. not identified
OSTI Identifier:
4202416
Patent Number(s):
2907631
Assignee:
U.S. Atomic Energy Commission
Patent Classifications (CPCs):
C - CHEMISTRY C01 - INORGANIC CHEMISTRY C01G - COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F
NSA Number:
NSA-14-007463
Resource Type:
Patent
Resource Relation:
Other Information: Orig. Receipt Date: 31-DEC-60
Country of Publication:
United States
Language:
English
Subject:
CHEMISTRY; ANIONS; BISMUTH PHOSPHATES; FISSION PRODUCTS; FLUORIDES; IONS; IRON; LANTHANUM FLUORIDES; NITRIC ACID; OXALATES; PHOSPHATES; PLUTONIUM; PLUTONIUM COMPLEXES; PRECIPITATION; SEPARATION PROCESSES; SOLUTIONS

Citation Formats

Dreher, J L, Koshland, D E, Thompson, S G, and Willard, J E. METHOD OF REDUCING PLUTONIUM WITH FERROUS IONS. United States: N. p., 1959. Web.
Dreher, J L, Koshland, D E, Thompson, S G, & Willard, J E. METHOD OF REDUCING PLUTONIUM WITH FERROUS IONS. United States.
Dreher, J L, Koshland, D E, Thompson, S G, and Willard, J E. Thu . "METHOD OF REDUCING PLUTONIUM WITH FERROUS IONS". United States.
@article{osti_4202416,
title = {METHOD OF REDUCING PLUTONIUM WITH FERROUS IONS},
author = {Dreher, J L and Koshland, D E and Thompson, S G and Willard, J E},
abstractNote = {A process is presented for separating hexavalent plutonium from fission product values. To a nitric acid solution containing the values, ferrous ions are added and the solution is heated and held at elevated temperature to convert the plutonium to the tetravalent state via the trivalent state and the plutonium is then selectively precipitated on a BiPO/sub 4/ or LaF/sub 3/ carrier. The tetravalent plutonium formed is optionally complexed with fluoride, oxalate, or phosphate anion prior to carrier precipitation.},
doi = {},
journal = {},
number = ,
volume = ,
place = {United States},
year = {1959},
month = {10}
}

Patent:
Search for the full text at the U.S. Patent and Trademark Office Note: You will be redirected to the USPTO site, which may require a pop-up blocker to be deactivated to view the patent. If so, you will need to manually turn off your browser's pop-up blocker, typically found within the browser settings. (See DOE Patents FAQs for more information.)

Save / Share: