SOLID STATE BONDING OF THORIUM WITH ALUMINUM
Abstract
A method is described for bonding thorium and aluminum by placing clean surfaces of thorium and aluminum in contact with each other and hot pressing the metals together in a protective atmosphere at a temperature of about 375 to 575 deg C and at a pressure of at least 10 tsi to effect a bond.
- Inventors:
- Issue Date:
- OSTI Identifier:
- 4195493
- Patent Number(s):
- 2914847
- Assignee:
- U.S. Atomic Energy Commission
- Patent Classifications (CPCs):
-
B - PERFORMING OPERATIONS B32 - LAYERED PRODUCTS B32B - LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- NSA Number:
- NSA-14-007756
- Resource Type:
- Patent
- Resource Relation:
- Other Information: Orig. Receipt Date: 31-DEC-60
- Country of Publication:
- United States
- Language:
- English
- Subject:
- METALS, CERAMICS, AND MATERIALS; ALUMINUM; BONDING; CLEANING; HIGH TEMPERATURE; INERT GASES; PRESSURE; SOLIDS; SURFACES; THORIUM
Citation Formats
Storchhelm, S. SOLID STATE BONDING OF THORIUM WITH ALUMINUM. United States: N. p., 1959.
Web.
Storchhelm, S. SOLID STATE BONDING OF THORIUM WITH ALUMINUM. United States.
Storchhelm, S. Tue .
"SOLID STATE BONDING OF THORIUM WITH ALUMINUM". United States.
@article{osti_4195493,
title = {SOLID STATE BONDING OF THORIUM WITH ALUMINUM},
author = {Storchhelm, S},
abstractNote = {A method is described for bonding thorium and aluminum by placing clean surfaces of thorium and aluminum in contact with each other and hot pressing the metals together in a protective atmosphere at a temperature of about 375 to 575 deg C and at a pressure of at least 10 tsi to effect a bond.},
doi = {},
journal = {},
number = ,
volume = ,
place = {United States},
year = {1959},
month = {12}
}