METHOD OF CONTROLLING CORROSION IN A NEUTRONIC REACTOR
Abstract
A method is described for reducing or removing corrosion and iron deposits on aluminum surfaces from coolant water comprising adding to the coolant alkali metal dichromate in a concentration of between 1.8 and 2.2 ppm, adjusting the pH to between 7.3 and 7.8 by adding CaCO/sub 3/ or other similar material, and adding a silicious material such as diatomaceous earth of a particle size of 5 to 15 microns to effect a suspension of between 2 and 300 ppm and circulating it through the reactor.
- Inventors:
- Issue Date:
- OSTI Identifier:
- 4174068
- Patent Number(s):
- 2907689
- Assignee:
- U.S. Atomic Energy Commission
- Patent Classifications (CPCs):
-
Y - NEW / CROSS SECTIONAL TECHNOLOGIES Y02 - TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE Y02E - REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
C - CHEMISTRY C23 - COATING METALLIC MATERIAL C23F - NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE
- NSA Number:
- NSA-14-007733
- Resource Type:
- Patent
- Resource Relation:
- Other Information: Orig. Receipt Date: 31-DEC-60
- Country of Publication:
- United States
- Language:
- English
- Subject:
- METALS, CERAMICS, AND MATERIALS; ACIDITY; ALKALI METALS; ALUMINUM; CALCIUM CARBONATES; CHROMATES; CORROSION; FILMS; GRAIN SIZE; IRON; OXIDES; SILICON OXIDES; SURFACES; SUSPENSIONS; WATER COOLANT
Citation Formats
Kidder, C P, and Sloan, C K. METHOD OF CONTROLLING CORROSION IN A NEUTRONIC REACTOR. United States: N. p., 1959.
Web.
Kidder, C P, & Sloan, C K. METHOD OF CONTROLLING CORROSION IN A NEUTRONIC REACTOR. United States.
Kidder, C P, and Sloan, C K. Thu .
"METHOD OF CONTROLLING CORROSION IN A NEUTRONIC REACTOR". United States.
@article{osti_4174068,
title = {METHOD OF CONTROLLING CORROSION IN A NEUTRONIC REACTOR},
author = {Kidder, C P and Sloan, C K},
abstractNote = {A method is described for reducing or removing corrosion and iron deposits on aluminum surfaces from coolant water comprising adding to the coolant alkali metal dichromate in a concentration of between 1.8 and 2.2 ppm, adjusting the pH to between 7.3 and 7.8 by adding CaCO/sub 3/ or other similar material, and adding a silicious material such as diatomaceous earth of a particle size of 5 to 15 microns to effect a suspension of between 2 and 300 ppm and circulating it through the reactor.},
doi = {},
journal = {},
number = ,
volume = ,
place = {United States},
year = {1959},
month = {10}
}