METHOD FOR ELECTRODEPOSITING POLONIUM
Abstract
The deposition of a thick uniform layer of polonium metal from aqueous solutions can be carried out by electrolyzing an aqueous solution of 1 N hydrofluoric acid containing about 0.13 curie of polonium per cubic centimeter of solution with platinum electrodes and a current density of about 1.2 ma/cm/sup 2/ of cathode surface.
- Inventors:
- Issue Date:
- OSTI Identifier:
- 4126605
- Patent Number(s):
- 2951020
- Assignee:
- U.S. Atomic Energy Commission
- Patent Classifications (CPCs):
-
C - CHEMISTRY C25 - ELECTROLYTIC OR ELECTROPHORETIC PROCESSES C25C - PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY OR REFINING OF METALS
C - CHEMISTRY C25 - ELECTROLYTIC OR ELECTROPHORETIC PROCESSES C25D - PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS
- NSA Number:
- NSA-14-025880
- Resource Type:
- Patent
- Resource Relation:
- Other Information: Orig. Receipt Date: 31-DEC-60
- Country of Publication:
- United States
- Language:
- English
- Subject:
- METALS, CERAMICS, AND OTHER MATERIALS; ELECTRODEPOSITION; ELECTRODES; ELECTROLYSIS; FILMS; HYDROFLUORIC ACID; PLATINUM; POLONIUM; SOLUTIONS; WATER
Citation Formats
Wehrmann, R F. METHOD FOR ELECTRODEPOSITING POLONIUM. United States: N. p., 1960.
Web.
Wehrmann, R F. METHOD FOR ELECTRODEPOSITING POLONIUM. United States.
Wehrmann, R F. Tue .
"METHOD FOR ELECTRODEPOSITING POLONIUM". United States.
@article{osti_4126605,
title = {METHOD FOR ELECTRODEPOSITING POLONIUM},
author = {Wehrmann, R F},
abstractNote = {The deposition of a thick uniform layer of polonium metal from aqueous solutions can be carried out by electrolyzing an aqueous solution of 1 N hydrofluoric acid containing about 0.13 curie of polonium per cubic centimeter of solution with platinum electrodes and a current density of about 1.2 ma/cm/sup 2/ of cathode surface.},
doi = {},
journal = {},
number = ,
volume = ,
place = {United States},
year = {1960},
month = {8}
}