GRAPHITE BONDING METHOD
Abstract
A process for bonding or joining graphite members together in which a thin platinum foil is placed between the members, heated in an inert atmosphere to a temperature of 1800 deg C, and then cooled to room temperature is described. (AEC)
- Inventors:
- Issue Date:
- Research Org.:
- Originating Research Org. not identified
- OSTI Identifier:
- 4112375
- Patent Number(s):
- 3122424
- Assignee:
- U.S. Atomic Energy Commission
- Patent Classifications (CPCs):
-
C - CHEMISTRY C04 - CEMENTS C04B - LIME, MAGNESIA
G - PHYSICS G21 - NUCLEAR PHYSICS G21C - NUCLEAR REACTORS
- NSA Number:
- NSA-18-010517
- Resource Type:
- Patent
- Resource Relation:
- Other Information: Orig. Receipt Date: 31-DEC-64
- Country of Publication:
- United States
- Language:
- English
- Subject:
- METALS, CERAMICS, AND OTHER MATERIALS; BONDING; COOLING; GRAPHITE; HEATING; HIGH TEMPERATURE; INERT GASES; JOINTS; PLATINUM; SHEETS; TEMPERATURE
Citation Formats
King, L D.P. GRAPHITE BONDING METHOD. United States: N. p., 1964.
Web.
King, L D.P. GRAPHITE BONDING METHOD. United States.
King, L D.P. Tue .
"GRAPHITE BONDING METHOD". United States.
@article{osti_4112375,
title = {GRAPHITE BONDING METHOD},
author = {King, L D.P.},
abstractNote = {A process for bonding or joining graphite members together in which a thin platinum foil is placed between the members, heated in an inert atmosphere to a temperature of 1800 deg C, and then cooled to room temperature is described. (AEC)},
doi = {},
journal = {},
number = ,
volume = ,
place = {United States},
year = {1964},
month = {2}
}
Search for the full text at the U.S. Patent and Trademark Office
Note: You will be redirected to the USPTO site, which may require a pop-up blocker to be deactivated to view the patent. If so, you will need to manually turn off your browser's pop-up blocker, typically found within the browser settings. (See DOE Patents FAQs for more information.)
Save to My Library
You must Sign In or Create an Account in order to save documents to your library.