Methods for using atomic layer deposition to produce a film for solid state electrolytes and protective electrode coatings for lithium batteries
Abstract
A method for using atomic layer deposition to produce a film configured for use in an anode, cathode, or solid state electrolyte of a lithium-ion battery or a lithium-sulfur battery. The method includes repeating a cycle for a predetermined number of times in an inert atmosphere. The cycle includes exposing a substrate to a first precursor, purging the substrate with inert gas, exposing the substrate to a second precursor, and purging the substrate with inert gas. The film is a metal sulfide.
- Inventors:
- Issue Date:
- Research Org.:
- Argonne National Laboratory (ANL), Argonne, IL (United States)
- Sponsoring Org.:
- USDOE
- OSTI Identifier:
- 1425947
- Patent Number(s):
- 9917295
- Application Number:
- 14/711,504
- Assignee:
- UChicago Argonne, LLC (Chicago, IL)
- Patent Classifications (CPCs):
-
H - ELECTRICITY H01 - BASIC ELECTRIC ELEMENTS H01M - PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
Y - NEW / CROSS SECTIONAL TECHNOLOGIES Y02 - TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE Y02E - REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- DOE Contract Number:
- AC02-06CH11357
- Resource Type:
- Patent
- Resource Relation:
- Patent File Date: 2015 May 13
- Country of Publication:
- United States
- Language:
- English
- Subject:
- 25 ENERGY STORAGE
Citation Formats
Elam, Jeffrey W., and Meng, Xiangbo. Methods for using atomic layer deposition to produce a film for solid state electrolytes and protective electrode coatings for lithium batteries. United States: N. p., 2018.
Web.
Elam, Jeffrey W., & Meng, Xiangbo. Methods for using atomic layer deposition to produce a film for solid state electrolytes and protective electrode coatings for lithium batteries. United States.
Elam, Jeffrey W., and Meng, Xiangbo. Tue .
"Methods for using atomic layer deposition to produce a film for solid state electrolytes and protective electrode coatings for lithium batteries". United States. https://www.osti.gov/servlets/purl/1425947.
@article{osti_1425947,
title = {Methods for using atomic layer deposition to produce a film for solid state electrolytes and protective electrode coatings for lithium batteries},
author = {Elam, Jeffrey W. and Meng, Xiangbo},
abstractNote = {A method for using atomic layer deposition to produce a film configured for use in an anode, cathode, or solid state electrolyte of a lithium-ion battery or a lithium-sulfur battery. The method includes repeating a cycle for a predetermined number of times in an inert atmosphere. The cycle includes exposing a substrate to a first precursor, purging the substrate with inert gas, exposing the substrate to a second precursor, and purging the substrate with inert gas. The film is a metal sulfide.},
doi = {},
journal = {},
number = ,
volume = ,
place = {United States},
year = {Tue Mar 13 00:00:00 EDT 2018},
month = {Tue Mar 13 00:00:00 EDT 2018}
}
Works referenced in this record:
Atomic layer deposition of metal sulfide thin films using non-halogenated precursors
patent, May 2015
- Martinson, Alex B.; Elam, Jeffrey W.; Pellin, Michael J.
- US Patent Document 9,040,113
Nanotechnological processing of catalytic surfaces
patent-application, June 2006
- Indech, Robert
- US Patent Application 11/051229; 20060115389
Integrated Electrochemical and Solar Cell
patent-application, March 2009
- Reynolds, Glyn
- US Patent Application 12/204338; 20090065042
Sulfur-Containing Thin Films
patent-application, June 2015
- Haukka, Suvi; Tang, Fu; Givens, Michael
- US Patent Application 14/133511; 20150170914
Atomic Layer Deposition of Lead Sulfide Quantum Dots on Nanowire Surfaces
journal, March 2011
- Dasgupta, Neil P.; Jung, Hee Joon; Trejo, Orlando
- Nano Letters, Vol. 11, Issue 3, p. 934-940
Design of an atomic layer deposition reactor for hydrogen sulfide compatibility
journal, April 2010
- Dasgupta, Neil P.; Mack, James F.; Langston, Michael C.
- Review of Scientific Instruments, Vol. 81, Issue 4, Article No. 044102
(Invited) Atomic Layer Deposition of Multicomponent Metal Sulfides Applied to Thin Film Photovoltaics
journal, August 2013
- Thimsen, E.
- ECS Transactions, Vol. 58, Issue 10, p. 95-104
Atomic Layer Deposition of Metal Sulfide Materials
journal, January 2015
- Dasgupta, Neil P.; Meng, Xiangbo; Elam, Jeffrey W.
- Accounts of Chemical Research, Vol. 48, Issue 2, p. 341-348
Gallium sulfide thin film grown on GaAs(1 0 0) by microwave glow discharge
journal, March 1997
- Chen, Xi-ying; Hou, Xiao-yuan; Cao, Xian-an
- Journal of Crystal Growth, Vol. 173, Issue 1-2, p. 51-56
Deposition of Thin Films of Gallium Sulfide from a Novel Single-Source Precursor, Ga(S2CNMeHex)3, by Low-Pressure Metal−Organic Chemical Vapor Deposition
journal, December 1999
- Lazell, Mike R.; O'Brien, Paul; Otway, David J.
- Chemistry of Materials, Vol. 11, Issue 12, p. 3430-3432
Growth, Optical and Structural Characterization of Layered GaS Films Prepared by Reactive RF Sputtering Method
journal, July 2005
- Ohyama, Masanori; Ito, Hiroshi; Takeuchi, Manabu
- Japanese Journal of Applied Physics, Vol. 44, Issue 7A, p. 4780-4783
Influence of the synthesis conditions on gallium sulfide thin films prepared by modulated flux deposition
journal, March 2009
- Sanz, C.; Guillén, C.; Gutiérrez, M. T.
- Journal of Physics D: Applied Physics, Vol. 42, Issue 8, Article No. 085108
Gallium (III) sulfide as an active material in lithium secondary batteries
journal, July 2011
- Senoh, Hiroshi; Kageyama, Hiroyuki; Takeuchi, Tomonari
- Journal of Power Sources, Vol. 196, Issue 13, p. 5631-5636
Chemical Vapor Deposition of Gallium Sulfide Thin Films
journal, September 2000
- Suh, Seigi; Hoffman, David M.
- Chemistry of Materials, Vol. 12, Issue 9, p. 2794-2797
Nanoporous Li2S and MWCNT-linked Li2S powder cathodes for lithium-sulfur and lithium-ion battery chemistries
journal, January 2014
- Wu, Feixiang; Magasinski, Alexandre; Yushin, Gleb
- Journal of Materials Chemistry A, Vol. 2, Issue 17, p. 6064-6070
High-Capacity Micrometer-Sized Li2 S Particles as Cathode Materials for Advanced Rechargeable Lithium-Ion Batteries
journal, September 2012
- Yang, Yuan; Zheng, Guangyuan; Misra, Sumohan
- Journal of the American Chemical Society, Vol. 134, Issue 37, p. 15387-15394
In situ synthesis of lithium sulfide–carbon composites as cathode materials for rechargeable lithium batteries
journal, January 2013
- Yang, Zichao; Guo, Juchen; Das, Shyamal K.
- Journal of Materials Chemistry A, Vol. 1, Issue 4, p. 1433-1440
Controlled Nucleation and Growth Process of Li2S2/Li2S in Lithium-Sulfur Batteries
journal, January 2013
- Zheng, Jianming; Gu, Meng; Wang, Chongmin
- Journal of The Electrochemical Society, Vol. 160, Issue 11, p. A1992-A1996