Title: Implantable devices having ceramic coating applied via an atomic layer deposition method

Abstract

Substrates coated with films of a ceramic material such as aluminum oxides and titanium oxides are biocompatible, and can be used in a variety of applications in which they are implanted in a living body. The substrate is preferably a porous polymer, and may be biodegradable. An important application for the ceramic-coated substrates is as a tissue engineering scaffold for forming artificial tissue.

Inventors:
; ;
Issue Date:
Research Org.:
The Regents of the University of Colorado, a Body Corporate, Denver, CO (United States)
Sponsoring Org.:
USDOE
OSTI Identifier:
1241323
Patent Number(s):
9,279,120
Application Number:
12/464,925
Assignee:
The Regents of the University of Colorado, a Body Corporate (Denver, CO)
DOE Contract Number:  
FG02-03ER86157
Resource Type:
Patent
Resource Relation:
Patent File Date: 2009 May 13
Country of Publication:
United States
Language:
English
Subject:
60 APPLIED LIFE SCIENCES; 59 BASIC BIOLOGICAL SCIENCES; 47 OTHER INSTRUMENTATION

Citation Formats

Liang, Xinhua, Weimer, Alan W., and Bryant, Stephanie J. Implantable devices having ceramic coating applied via an atomic layer deposition method. United States: N. p., 2016. Web.
Liang, Xinhua, Weimer, Alan W., & Bryant, Stephanie J. Implantable devices having ceramic coating applied via an atomic layer deposition method. United States.
Liang, Xinhua, Weimer, Alan W., and Bryant, Stephanie J. Tue . "Implantable devices having ceramic coating applied via an atomic layer deposition method". United States. https://www.osti.gov/servlets/purl/1241323.
@article{osti_1241323,
title = {Implantable devices having ceramic coating applied via an atomic layer deposition method},
author = {Liang, Xinhua and Weimer, Alan W. and Bryant, Stephanie J.},
abstractNote = {Substrates coated with films of a ceramic material such as aluminum oxides and titanium oxides are biocompatible, and can be used in a variety of applications in which they are implanted in a living body. The substrate is preferably a porous polymer, and may be biodegradable. An important application for the ceramic-coated substrates is as a tissue engineering scaffold for forming artificial tissue.},
doi = {},
journal = {},
number = ,
volume = ,
place = {United States},
year = {2016},
month = {3}
}

Patent:

Save / Share:

Works referenced in this record:

Biodegradable and bioactive porous polymer/inorganic composite scaffolds for bone tissue engineering
journal, June 2006


Poly(D,L-lactide) (PDLLA) foams with TiO2 nanoparticles and PDLLA/TiO2-Bioglass® foam composites for tissue engineering scaffolds
journal, July 2006

  • Boccaccini, Aldo R.; Blaker, Jonny J.; Maquet, Véronique
  • Journal of Materials Science, Vol. 41, Issue 13
  • DOI: 10.1007/s10853-006-7575-7