Alloy substantially free of dendrites and method of forming the same
Patent
·
OSTI ID:986525
- West Newton, MA
- West Boylston, MA
- Monson, MA
- S. Windson, CT
Described herein are alloys substantially free of dendrites. A method includes forming an alloy substantially free of dendrites. A superheated alloy is cooled to form a nucleated alloy. The temperature of the nucleated alloy is controlled to prevent the nuclei from melting. The nucleated alloy is mixed to distribute the nuclei throughout the alloy. The nucleated alloy is cooled with nuclei distributed throughout.
- Research Organization:
- Worcester Polytechnic Institute, Worcester, MA (United States)
- Sponsoring Organization:
- USDOE
- DOE Contract Number:
- FC36-02ID14232
- Assignee:
- Worcester Polytechnic Institute (Worcester, MA)
- Patent Number(s):
- 7,513,962
- Application Number:
- 10/668,668; TRN: US201017%%386
- OSTI ID:
- 986525
- Country of Publication:
- United States
- Language:
- English
Similar Records
Energy Saving Melting and Revert Reduction Technology: Innovative Semi-Solid Metal (SSM) Processing
Large single crystal quaternary alloys of IB-IIIA-SE.sub.2 and methods of synthesizing the same
Large single crystal quaternary alloys of IB-IIIA-Se/sub 2/ and methods of synthesizing the same
Technical Report
·
Wed Aug 15 00:00:00 EDT 2012
·
OSTI ID:986525
Large single crystal quaternary alloys of IB-IIIA-SE.sub.2 and methods of synthesizing the same
Patent
·
Fri Jan 01 00:00:00 EST 1988
·
OSTI ID:986525
Large single crystal quaternary alloys of IB-IIIA-Se/sub 2/ and methods of synthesizing the same
Patent
·
Tue Jul 15 00:00:00 EDT 1986
·
OSTI ID:986525