Title: Methods of forming aluminum oxynitride-comprising bodies, including methods of forming a sheet of transparent armor

Abstract

The invention includes methods of forming an aluminum oxynitride-comprising body. For example, a mixture is formed which comprises A:B:C in a respective molar ratio in the range of 9:3.6-6.2:0.1-1.1, where "A" is Al.sub.2O.sub.3, "B" is AlN, and "C" is a total of one or more of B.sub.2O.sub.3, SiO.sub.2, Si--Al--O--N, and TiO.sub.2. The mixture is sintered at a temperature of at least 1,600.degree. C. at a pressure of no greater than 500 psia effective to form an aluminum oxynitride-comprising body which is at least internally transparent and has at least 99% maximum theoretical density.

Inventors:
 [1];  [1]
  1. Idaho Falls, ID
Publication Date:
Research Org.:
Idaho National Lab. (INL), Idaho Falls, ID (United States)
Sponsoring Org.:
USDOE
OSTI Identifier:
985725
Patent Number(s):
7,459,122
Application Number:
11/427,840
Assignee:
Battelle Energy Alliance, LLC (Idaho Falls, ID) IDO
DOE Contract Number:  
AC07-05ID14517
Resource Type:
Patent
Country of Publication:
United States
Language:
English
Subject:
37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CHEMISTRY; 36 MATERIALS SCIENCE

Citation Formats

Chu, Henry Shiu-Hung, and Lillo, Thomas Martin. Methods of forming aluminum oxynitride-comprising bodies, including methods of forming a sheet of transparent armor. United States: N. p., 2008. Web.
Chu, Henry Shiu-Hung, & Lillo, Thomas Martin. Methods of forming aluminum oxynitride-comprising bodies, including methods of forming a sheet of transparent armor. United States.
Chu, Henry Shiu-Hung, and Lillo, Thomas Martin. Tue . "Methods of forming aluminum oxynitride-comprising bodies, including methods of forming a sheet of transparent armor". United States. https://www.osti.gov/servlets/purl/985725.
@article{osti_985725,
title = {Methods of forming aluminum oxynitride-comprising bodies, including methods of forming a sheet of transparent armor},
author = {Chu, Henry Shiu-Hung and Lillo, Thomas Martin},
abstractNote = {The invention includes methods of forming an aluminum oxynitride-comprising body. For example, a mixture is formed which comprises A:B:C in a respective molar ratio in the range of 9:3.6-6.2:0.1-1.1, where "A" is Al.sub.2O.sub.3, "B" is AlN, and "C" is a total of one or more of B.sub.2O.sub.3, SiO.sub.2, Si--Al--O--N, and TiO.sub.2. The mixture is sintered at a temperature of at least 1,600.degree. C. at a pressure of no greater than 500 psia effective to form an aluminum oxynitride-comprising body which is at least internally transparent and has at least 99% maximum theoretical density.},
doi = {},
journal = {},
number = ,
volume = ,
place = {United States},
year = {2008},
month = {12}
}

Patent:

Save / Share: