MgAl2O4 spinel refractory as containment liner for high-temperature alkali salt containing environments
Patent
·
OSTI ID:985347
- Knoxville, TN
- Oak Ridge, TN
- Kent, WA
- Jamestown, NY
A method includes containing a high-temperature alkali salt containing environment using a refractory containment liner containing MgAl.sub.2O.sub.4 spinel. A method, includes forming a refractory brick containing MgAl.sub.2O.sub.4 spinel having an exterior chill zone defined by substantially columnar crystallization and an interior zone defined by substantially equiaxed crystallization; and removing at least a portion of the exterior chill zone from the refractory brick containing MgAl.sub.2O.sub.4 spinel by scalping the refractory brick containing MgAl.sub.2O.sub.4 spinel to define at least one outer surface having an area of substantially equiaxed crystallization. A product of manufacture includes a refractory brick containing MgAl.sub.2O.sub.4 spinel including an interior zone defined by substantially equiaxed crystallization; and at least one outer surface having an area of substantially equiaxed crystallization.
- Research Organization:
- Oak Ridge National Laboratory (ORNL), Oak Ridge, TN (United States)
- Sponsoring Organization:
- USDOE
- DOE Contract Number:
- AC05-00OR22725
- Assignee:
- UT-Battelle, LLC (Oak Ridge, TN)
- Patent Number(s):
- 7,438,004
- Application Number:
- 11/207,320
- OSTI ID:
- 985347
- Country of Publication:
- United States
- Language:
- English
| Study of mixed á/â-alumina and pure â-alumina fused cast refractories after exposure in the black liquor gasifier in New Bern, North Carolina. CRADA final report | report | March 1999 |
Reaction of molten sodium carbonate with aluminum oxide
|
journal | January 1978 |
Similar Records
Chromia refractory brick with carbon treatment
Alkali metal battery structure
Alkali Vapor Corrosion of Spinel (MgAl2O4) and Gahnite (ZnAl2O4) Refractories—A Comparative Study
Patent
·
2017
·
OSTI ID:1347592
Alkali metal battery structure
Patent
·
1977
·
OSTI ID:7279150
Alkali Vapor Corrosion of Spinel (MgAl2O4) and Gahnite (ZnAl2O4) Refractories—A Comparative Study
Journal Article
·
2026
· Journal of the American Ceramic Society
·
OSTI ID:3364711