EFFECTS OF CHEMISTRY AND OTHER VARIABLES ON CORROSION AND STRESS CORROSION CRACKING IN HANFORD DOUBLE SHELL TANKS
Laboratory testing was performed to develop a comprehensive understanding of the corrosivity of the tank wastes stored in Double-Shell Tanks using simulants primarily from Tanks 241-AP-105, 241-SY-103 and 241-AW-105. Additional tests were conducted using simulants of the waste stored in 241-AZ-102, 241-SY-101, 241-AN-107, and 241-AY-101. This test program placed particular emphasis on defining the range of tank waste chemistries that do not induce the onset of localized forms of corrosion, particularly pitting and stress corrosion cracking. This document summarizes the key findings of the research program.
- Research Organization:
- Hanford Site (HNF), Richland, WA (United States)
- Sponsoring Organization:
- USDOE Assistant Secretary for Environmental Management (EM)
- DOE Contract Number:
- DE-AC27-08RV14800
- OSTI ID:
- 943299
- Report Number(s):
- RPP-RPT-37505 Rev 0; TRN: US0900392
- Country of Publication:
- United States
- Language:
- English
Similar Records
Hanford Double-Shell Tank Extent-of-Condition Construction Review
CESIUM REMOVAL FROM TANKS 241-AN-103 & 241-SX-105 & 241-AZ-101 & 241AZ-102 COMPOSITE FOR TESTING IN BENCH SCALE STEAM REFORMER
CESIUM REMOVAL FROM TANKS 241-AN-103 & 241-SX-105 & 241-AZ-101/102 COMPOSITE FOR TESTING IN BENCH SCALE STEAM REFORMER
Conference
·
Thu Nov 14 00:00:00 EST 2013
·
OSTI ID:943299
+3 more
CESIUM REMOVAL FROM TANKS 241-AN-103 & 241-SX-105 & 241-AZ-101 & 241AZ-102 COMPOSITE FOR TESTING IN BENCH SCALE STEAM REFORMER
Technical Report
·
Thu Apr 21 00:00:00 EDT 2011
·
OSTI ID:943299
CESIUM REMOVAL FROM TANKS 241-AN-103 & 241-SX-105 & 241-AZ-101/102 COMPOSITE FOR TESTING IN BENCH SCALE STEAM REFORMER
Technical Report
·
Wed Jun 08 00:00:00 EDT 2011
·
OSTI ID:943299