Title: Dynamic and static measurements of elastic constants with data on 2 1/4 Cr--1 Mo steel, types 304 and 316 stainless steels, and alloy 800H

Abstract

Methods for determining the dynamic and static elastic constants (E, G, and ..nu..) of engineering materials were developed and evaluated. A hybrid sonic method incorporating the double pulse, block-sample technique for determining accurate room-temperature data and the single pulse, thin-wire technique for gathering elevated-temperature data were used to determine the dynamic elastic constants. Of three methods examined for measuring static constants (using the linear variable differential transformer, the weldable resistance gage, and the capacitive gage), the method employing the linear variable differential transformer gage served well as a reference method for dtermining Young' modulus. The method using the capacitive gage showed greatest merit for determining combined E, G, and ..nu... The dynamic and static elastic constants of 2 1/4 Cr--1 Mo steel, types 304- and 316 stainless steel, and alloy 800H were determined from room temperature to 649/sup 0/C (1200/sup 0/F) and higher.

Authors:
; ; ; ;
Publication Date:
Research Org.:
Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States)
Sponsoring Org.:
USDOE
OSTI Identifier:
6216499
Report Number(s):
ORNL-5442
DOE Contract Number:  
W-7405-ENG-26
Resource Type:
Technical Report
Country of Publication:
United States
Language:
English
Subject:
36 MATERIALS SCIENCE; CHROMIUM-MOLYBDENUM STEELS; POISSON RATIO; SHEAR PROPERTIES; YOUNG MODULUS; INCOLOY 800; STAINLESS STEEL-304; STAINLESS STEEL-316; ALLOYS; CHROMIUM ALLOYS; CHROMIUM STEELS; CHROMIUM-NICKEL STEELS; CORROSION RESISTANT ALLOYS; ELASTICITY; HEAT RESISTANT MATERIALS; HEAT RESISTING ALLOYS; INCOLOY ALLOYS; IRON ALLOYS; IRON BASE ALLOYS; MATERIALS; MECHANICAL PROPERTIES; MOLYBDENUM ALLOYS; NICKEL ALLOYS; STAINLESS STEELS; STEELS; TENSILE PROPERTIES; 360103* - Metals & Alloys- Mechanical Properties

Citation Formats

Hammond, J P, Ratcliff, L T, Brinkman, C R, Moyer, M W, and Nestor, Jr, C W. Dynamic and static measurements of elastic constants with data on 2 1/4 Cr--1 Mo steel, types 304 and 316 stainless steels, and alloy 800H. United States: N. p., 1979. Web. doi:10.2172/6216499.
Hammond, J P, Ratcliff, L T, Brinkman, C R, Moyer, M W, & Nestor, Jr, C W. Dynamic and static measurements of elastic constants with data on 2 1/4 Cr--1 Mo steel, types 304 and 316 stainless steels, and alloy 800H. United States. doi:10.2172/6216499.
Hammond, J P, Ratcliff, L T, Brinkman, C R, Moyer, M W, and Nestor, Jr, C W. Thu . "Dynamic and static measurements of elastic constants with data on 2 1/4 Cr--1 Mo steel, types 304 and 316 stainless steels, and alloy 800H". United States. doi:10.2172/6216499. https://www.osti.gov/servlets/purl/6216499.
@article{osti_6216499,
title = {Dynamic and static measurements of elastic constants with data on 2 1/4 Cr--1 Mo steel, types 304 and 316 stainless steels, and alloy 800H},
author = {Hammond, J P and Ratcliff, L T and Brinkman, C R and Moyer, M W and Nestor, Jr, C W},
abstractNote = {Methods for determining the dynamic and static elastic constants (E, G, and ..nu..) of engineering materials were developed and evaluated. A hybrid sonic method incorporating the double pulse, block-sample technique for determining accurate room-temperature data and the single pulse, thin-wire technique for gathering elevated-temperature data were used to determine the dynamic elastic constants. Of three methods examined for measuring static constants (using the linear variable differential transformer, the weldable resistance gage, and the capacitive gage), the method employing the linear variable differential transformer gage served well as a reference method for dtermining Young' modulus. The method using the capacitive gage showed greatest merit for determining combined E, G, and ..nu... The dynamic and static elastic constants of 2 1/4 Cr--1 Mo steel, types 304- and 316 stainless steel, and alloy 800H were determined from room temperature to 649/sup 0/C (1200/sup 0/F) and higher.},
doi = {10.2172/6216499},
journal = {},
number = ,
volume = ,
place = {United States},
year = {1979},
month = {2}
}