Title: Fractography of glasses and ceramics

Abstract

This book collects papers on fracture mechanics in vitreous and ceramic materials. Topics include: crack branching in ceramics, fractographic determination of crack-tip stress intensity, fracture mechanisms of solid-state slab lasers, beta alumina failure in sodium-sulfur batteries, and fractography of glass.

Authors:
;
Publication Date:
OSTI Identifier:
5929123
Alternate Identifier(s):
OSTI ID: 5929123
Report Number(s):
CONF-8608230-
Resource Type:
Conference
Resource Relation:
Conference: Fractography of glasses and ceramics, Alfred, NY, USA, 3 Aug 1986; Related Information: Advances in Ceramics. Volume 22
Country of Publication:
United States
Language:
English
Subject:
36 MATERIALS SCIENCE; 25 ENERGY STORAGE; 42 ENGINEERING; ALUMINIUM OXIDES; FRACTURE MECHANICS; CERAMICS; ELECTROLYTES; TUBES; GLASS; LASER MATERIALS; SODIUM-SULFUR BATTERIES; CRACK PROPAGATION; LEADING ABSTRACT; STRESS ANALYSIS; STRESS INTENSITY FACTORS; ABSTRACTS; ALUMINIUM COMPOUNDS; CHALCOGENIDES; DOCUMENT TYPES; ELECTRIC BATTERIES; ELECTROCHEMICAL CELLS; MATERIALS; MECHANICS; METAL-NONMETAL BATTERIES; OXIDES; OXYGEN COMPOUNDS 360203* -- Ceramics, Cermets, & Refractories-- Mechanical Properties; 360603 -- Materials-- Properties; 250903 -- Energy Storage-- Batteries-- Materials, Components, & Auxiliaries; 420300 -- Engineering-- Lasers-- (-1989)

Citation Formats

Frechette, V.D., and Varner, J.R. Fractography of glasses and ceramics. United States: N. p., 1988. Web.
Frechette, V.D., & Varner, J.R. Fractography of glasses and ceramics. United States.
Frechette, V.D., and Varner, J.R. Fri . "Fractography of glasses and ceramics". United States.
@article{osti_5929123,
title = {Fractography of glasses and ceramics},
author = {Frechette, V.D. and Varner, J.R.},
abstractNote = {This book collects papers on fracture mechanics in vitreous and ceramic materials. Topics include: crack branching in ceramics, fractographic determination of crack-tip stress intensity, fracture mechanisms of solid-state slab lasers, beta alumina failure in sodium-sulfur batteries, and fractography of glass.},
doi = {},
journal = {},
number = ,
volume = ,
place = {United States},
year = {1988},
month = {1}
}

Conference:
Other availability
Please see Document Availability for additional information on obtaining the full-text document. Library patrons may search WorldCat to identify libraries that hold this conference proceeding.

Save / Share: