STRUCTURAL MATERIALS AND WELDING FOR STEAM GENERATORS IN SODIUM-COOLED FAST BREEDER REACTORS. (in Japanese)
Journal Article
·
· FAPIG (Tokyo), No. 53, 52-61(May 1969).
OSTI ID:4746408
- Research Organization:
- Kawasaki Dockyard Co., Kobe, Japan
- NSA Number:
- NSA-24-001029
- OSTI ID:
- 4746408
- Journal Information:
- FAPIG (Tokyo), No. 53, 52-61(May 1969)., Other Information: Orig. Receipt Date: 31-DEC-70; Bib. Info. Source: NSAJ (NSA of Japan)
- Country of Publication:
- Country unknown/Code not available
- Language:
- Japanese
Similar Records
Steam generator material for sodium-cooled fast breeder reactors: results and future prospects
Steam generator material for sodium-cooled fast breeder reactors. Results and future prospects
AI-TYPE STEAM GENERATOR FOR A PROTOTYPE SODIUM-COOLED FAST BREEDER REACTOR.
Journal Article
·
Tue Apr 01 00:00:00 EDT 1975
· Trans. Am. Nucl. Soc., v. 20, pp. 86-89
·
OSTI ID:4746408
+6 more
Steam generator material for sodium-cooled fast breeder reactors. Results and future prospects
Conference
·
Wed Jan 01 00:00:00 EST 1975
·
OSTI ID:4746408
+4 more
AI-TYPE STEAM GENERATOR FOR A PROTOTYPE SODIUM-COOLED FAST BREEDER REACTOR.
Journal Article
·
Wed Jan 01 00:00:00 EST 1969
· FAPIG (Tokyo) No. 55, 158-64(Dec 1969).
·
OSTI ID:4746408
Related Subjects
N30130* -Metals
Ceramics
& Other Materials-Metals & Alloys-Properties Evaluations
N30120 -Metals
Ceramics
& Other Materials-Metals & Alloys-Preparation & Fabrication
N38890 -Commercial Power Reactors-Steam & Power Conversion Systems
BOILERS
BOILING
BREEDER REACTORS
CHROMIUM STEELS- MOLYBDENUM
DESIGN
FAST REACTORS
MATERIALS TESTING
MECHANICAL PROPERTIES
METAL COOLED REACTORS
STEAM
STEAM GENERATORS
WELDING AUSTENITE- STAINLESS STEELS
STAINLESS STEEL/welding of austenitic
CHROMIUM ALLOYS AND SYSTEMS/Cr-Mo-steel
mechanical properties and welding of
BOILERS/design, fabrication, and materials selection for sodium-cooled fast breeder-reactor
LIQUID METAL FAST BREEDER REACTOR/steam generators for, design, fabrication, and materials selection for
STEEL/Cr-Mo-steel
mechanical properties and welding of
STAINLESS STEEL/mechanical properties of austenitic
MOLYBDENUM ALLOYS AND SYSTEMS/Cr-Mo-steel
mechanical properties and welding of
Ceramics
& Other Materials-Metals & Alloys-Properties Evaluations
N30120 -Metals
Ceramics
& Other Materials-Metals & Alloys-Preparation & Fabrication
N38890 -Commercial Power Reactors-Steam & Power Conversion Systems
BOILERS
BOILING
BREEDER REACTORS
CHROMIUM STEELS- MOLYBDENUM
DESIGN
FAST REACTORS
MATERIALS TESTING
MECHANICAL PROPERTIES
METAL COOLED REACTORS
STEAM
STEAM GENERATORS
WELDING AUSTENITE- STAINLESS STEELS
STAINLESS STEEL/welding of austenitic
CHROMIUM ALLOYS AND SYSTEMS/Cr-Mo-steel
mechanical properties and welding of
BOILERS/design, fabrication, and materials selection for sodium-cooled fast breeder-reactor
LIQUID METAL FAST BREEDER REACTOR/steam generators for, design, fabrication, and materials selection for
STEEL/Cr-Mo-steel
mechanical properties and welding of
STAINLESS STEEL/mechanical properties of austenitic
MOLYBDENUM ALLOYS AND SYSTEMS/Cr-Mo-steel
mechanical properties and welding of