GALVANIC CORROSION OF AUSTENITIC Fe--Cr--Ni ALLOYS IN NITRIC MEDIA. BEHAVIOR OF Fe--Cr--Ni AUSTENITIC ALLOYS IN THE TRANSPASSIVATION REGION. (in French)
Journal Article
·
· Mem. Sci. Rev. Met. 68: No. 7, 489-97(Jul 1971).
OSTI ID:4706685
- Research Organization:
- CEN, Fontenay-aux-Roses, France; and others
- NSA Number:
- NSA-26-002465
- OSTI ID:
- 4706685
- Journal Information:
- Mem. Sci. Rev. Met. 68: No. 7, 489-97(Jul 1971)., Other Information: Orig. Receipt Date: 31-DEC-72
- Country of Publication:
- France
- Language:
- French
Similar Records
Comparative study of stress corrosion tests for austenitic, austeno- ferritic and ferritic Fe-Cr-Ni and Fe-Cr alloys in chloride media. Influence of steel composition and structure. Influence of the chemical properties of the corrosive medium. Comparison with the results found in industrial practice
CORROSION PROBLEMS ARISING FROM THE USE OF AUSTENITIC Cr--Ni--Fe ALLOYS IN NUCLEAR APPLICATIONS.
STUDIES OF THE TENDENCY OF INTERGRANULAR CORROSION CRACKING OF AUSTENITIC Fe--Cr--Ni ALLOYS IN HIGH PURITY WATER AT 300$sup 0$C.
Conference
·
Sun Dec 01 00:00:00 EST 1974
· Mem. Sci. Rev. Metall., v. 71, no. 12, pp. 807-822
·
OSTI ID:4706685
+2 more
CORROSION PROBLEMS ARISING FROM THE USE OF AUSTENITIC Cr--Ni--Fe ALLOYS IN NUCLEAR APPLICATIONS.
Journal Article
·
Sun Jan 01 00:00:00 EST 1967
· Energ. Nucl. (Paris), 9: 303-13 (Aug.-Sept. 1967).
·
OSTI ID:4706685
STUDIES OF THE TENDENCY OF INTERGRANULAR CORROSION CRACKING OF AUSTENITIC Fe--Cr--Ni ALLOYS IN HIGH PURITY WATER AT 300$sup 0$C.
Technical Report
·
Fri Jan 01 00:00:00 EST 1971
·
OSTI ID:4706685
Related Subjects
N30110* -Metals
Ceramics
& Other Materials-Metals & Alloys-Corrosion & Erosion & Surface Phenomena
AUSTENITE
CHROMIUM ALLOYS
COUPLING
GRAPHITE
INTERGRANULAR CORROSION
IRON ALLOYS
NICKEL ALLOYS
NITRIC ACID
PASSIVATION
STEELS
CHROMIUM ALLOYS AND SYSTEMS/Cr-Ni-steel
corrosion by nitric acid
galvanic
STEEL COUPLES/graphite/steel
corrosion by nitric acid
galvanic
NITRIC ACID/corrosive effects on chromium-steel, graphite/steel couples, nickel-steel, and chromium-nickel steel in transpassivation region
STEEL/Cr-steel
corrosion by nitric acid
galvanic
STEEL/Cr-Ni-steel
corrosion by nitric acid
galvanic
CHROMIUM ALLOYS AND SYSTEMS/Cr-steel
corrosion by nitric acid
galvanic
NICKEL ALLOYS AND SYSTEMS/Cr-Ni-steel
corrosion by nitric acid
galvanic
GRAPHITE COUPLES/graphite/steel
corrosion by nitric acid
galvanic
NICKEL ALLOYS AND SYSTEMS/Ni-steel
corrosion by nitric acid
galvanic
STEEL/Ni-steel
corrosion by nitric acid
galvanic
Ceramics
& Other Materials-Metals & Alloys-Corrosion & Erosion & Surface Phenomena
AUSTENITE
CHROMIUM ALLOYS
COUPLING
GRAPHITE
INTERGRANULAR CORROSION
IRON ALLOYS
NICKEL ALLOYS
NITRIC ACID
PASSIVATION
STEELS
CHROMIUM ALLOYS AND SYSTEMS/Cr-Ni-steel
corrosion by nitric acid
galvanic
STEEL COUPLES/graphite/steel
corrosion by nitric acid
galvanic
NITRIC ACID/corrosive effects on chromium-steel, graphite/steel couples, nickel-steel, and chromium-nickel steel in transpassivation region
STEEL/Cr-steel
corrosion by nitric acid
galvanic
STEEL/Cr-Ni-steel
corrosion by nitric acid
galvanic
CHROMIUM ALLOYS AND SYSTEMS/Cr-steel
corrosion by nitric acid
galvanic
NICKEL ALLOYS AND SYSTEMS/Cr-Ni-steel
corrosion by nitric acid
galvanic
GRAPHITE COUPLES/graphite/steel
corrosion by nitric acid
galvanic
NICKEL ALLOYS AND SYSTEMS/Ni-steel
corrosion by nitric acid
galvanic
STEEL/Ni-steel
corrosion by nitric acid
galvanic