Title: METALLURGICAL INVESTIGATIONS ON THE CLADDING FAILURE IN THE JPDR PRESSURE VESSEL. II. A STUDY ON THE PITTING CORROSION IN HIGH TEMPERATURE WATER OF A LOW ALLOY STEEL WITHIN THE SIMULATED CRACKS IN THE PROTECTIVE WELD OVERLAY. (in Japanese)

Authors:
; ; ;
Publication Date:
Research Org.:
Japan Atomic Energy Research Inst., Tokyo
OSTI Identifier:
4642074
Report Number(s):
JAERI-Memo-4019
NSA Number:
NSA-26-048358
Resource Type:
Technical Report
Resource Relation:
Other Information: UNCL. Orig. Receipt Date: 31-DEC-72
Country of Publication:
Japan
Language:
Japanese
Subject:
N50210* -Metals, Ceramics, & Other Materials-Metals & Alloys-Corrosion & Erosion & Surface Phenomena; N78241 -Power Reactor Development-Commercial Power Reactors-Cooling Systems-Non-breeder Boiling Water; COOLANTS; CORROSION; FAILURES; JPDR REACTOR; PRESSURE VESSELS; STAINLESS STEELS; STEELS; SURFACE COATING; WATER; WATER COOLED REACTORS; WELDS; STEEL/corrosion of JPDR pressure vessel, by high- temperature coolant water following failure of stainless steel cladding; STAINLESS STEEL/failure of JPDR pressure vessel cladding of, pitting corrosion of steel base by high-temperature coolant water following; JAPANESE POWER DEMONSTRATION REACTOR/pressure vessel corrosion by coolant water in, following stainless steel cladding failure

Citation Formats

Kondo, T, Nagasaki, R, Shimizu, Y, and Ito, G. METALLURGICAL INVESTIGATIONS ON THE CLADDING FAILURE IN THE JPDR PRESSURE VESSEL. II. A STUDY ON THE PITTING CORROSION IN HIGH TEMPERATURE WATER OF A LOW ALLOY STEEL WITHIN THE SIMULATED CRACKS IN THE PROTECTIVE WELD OVERLAY.. Japan: N. p., 1970. Web.
Kondo, T, Nagasaki, R, Shimizu, Y, & Ito, G. METALLURGICAL INVESTIGATIONS ON THE CLADDING FAILURE IN THE JPDR PRESSURE VESSEL. II. A STUDY ON THE PITTING CORROSION IN HIGH TEMPERATURE WATER OF A LOW ALLOY STEEL WITHIN THE SIMULATED CRACKS IN THE PROTECTIVE WELD OVERLAY.. Japan.
Kondo, T, Nagasaki, R, Shimizu, Y, and Ito, G. Thu . "METALLURGICAL INVESTIGATIONS ON THE CLADDING FAILURE IN THE JPDR PRESSURE VESSEL. II. A STUDY ON THE PITTING CORROSION IN HIGH TEMPERATURE WATER OF A LOW ALLOY STEEL WITHIN THE SIMULATED CRACKS IN THE PROTECTIVE WELD OVERLAY.". Japan.
@article{osti_4642074,
title = {METALLURGICAL INVESTIGATIONS ON THE CLADDING FAILURE IN THE JPDR PRESSURE VESSEL. II. A STUDY ON THE PITTING CORROSION IN HIGH TEMPERATURE WATER OF A LOW ALLOY STEEL WITHIN THE SIMULATED CRACKS IN THE PROTECTIVE WELD OVERLAY.},
author = {Kondo, T and Nagasaki, R and Shimizu, Y and Ito, G},
abstractNote = {},
doi = {},
journal = {},
number = ,
volume = ,
place = {Japan},
year = {1970},
month = {1}
}

Technical Report:
Other availability
Please see Document Availability for additional information on obtaining the full-text document. Library patrons may search WorldCat to identify libraries that may hold this item. Keep in mind that many technical reports are not cataloged in WorldCat.

Save / Share: