AQUEOUS STRESS CORROSION CRACKING AND STRESS CORROSION FATIGUE OF A HIGH STRENGTH TITANIUM ALLOY.
Journal Article
·
· pp 613-21 of Space Shuttle Materials. Vol. 3. Azusa, Calif. Society of Aerospace Material and Process Engineers (1971).
OSTI ID:4613571
- Research Organization:
- North American Rockwell Science Center, Thousand Oaks, Calif.
- NSA Number:
- NSA-27-010006
- OSTI ID:
- 4613571
- Journal Information:
- pp 613-21 of Space Shuttle Materials. Vol. 3. Azusa, Calif. Society of Aerospace Material and Process Engineers (1971)., Other Information: From National SAMPE conference; Huntsville, AL. (5 Oct 1971). See CONF- 711054--(Vol.3). Orig. Receipt Date: 30-JUN-73
- Country of Publication:
- Country unknown/Code not available
- Language:
- English
Similar Records
STRESS-CORROSION CRACKING OF HIGH STRENGTH STEELS AND TITANIUM ALLOYS.
On ripple-load, stress-corrosion, and sustained-load cracking behavior in a high strength beta titanium alloy
STRESS-CORROSION CRACKING OF HIGH-STRENGTH STEELS AND TITANIUM ALLOYS.
Journal Article
·
Sat Jan 01 00:00:00 EST 1972
· Weld. J. (N. Y.) 51: No. 9, 437s-48s(Sep 1972).
·
OSTI ID:4613571
On ripple-load, stress-corrosion, and sustained-load cracking behavior in a high strength beta titanium alloy
Journal Article
·
Sun Jun 01 00:00:00 EDT 1997
· Scripta Materialia
·
OSTI ID:4613571
+2 more
STRESS-CORROSION CRACKING OF HIGH-STRENGTH STEELS AND TITANIUM ALLOYS.
Technical Report
·
Fri Jan 01 00:00:00 EST 1971
·
OSTI ID:4613571
Related Subjects
N50230* -Metals
Ceramics
& Other Materials-Metals & Alloys-Properties
Structure & Phase Studies
ALUMINIUM ALLOYS
CRACKS
ELECTROCHEMISTRY
MICROSTRUCTURE
MOLYBDENUM ALLOYS
STRESS CORROSION
STRESSES
TIN ALLOYS
TITANIUM BASE ALLOYS
ZIRCONIUM ALLOYS
ZIRCONIUM ALLOYS AND SYSTEMS/Al-Mo-Sn-Ti-base-Zr, stress corrosion cracking of, effects of electrochemical potential, microstructure, and stress intensity factor on
ALUMINUM ALLOYS AND SYSTEMS/Al- Mo-Sn-Ti-base-Zr, stress corrosion cracking of, effects of electrochemical potential, microstructure, and stress intensity factor on
TIN ALLOYS AND SYSTEMS/ Al-Mo-Sn-Ti-base-Zr, stress corrosion cracking of, effects of electrochemical potential, microstructure, and stress intensity factor on
TITANIUM ALLOYS AND SYSTEMS/Al-Mo-Sn-Ti-base-Zr, stress corrosion cracking of, effects of electrochemical potential, microstructure, and stress intensity factor on
MOLYBDENUM ALLOYS AND SYSTEMS/Al-Mo-Sn-Ti-base-Zr, stress corrosion cracking of, effects of electrochemical potential, microstructure, and stress intensity factor on
Ceramics
& Other Materials-Metals & Alloys-Properties
Structure & Phase Studies
ALUMINIUM ALLOYS
CRACKS
ELECTROCHEMISTRY
MICROSTRUCTURE
MOLYBDENUM ALLOYS
STRESS CORROSION
STRESSES
TIN ALLOYS
TITANIUM BASE ALLOYS
ZIRCONIUM ALLOYS
ZIRCONIUM ALLOYS AND SYSTEMS/Al-Mo-Sn-Ti-base-Zr, stress corrosion cracking of, effects of electrochemical potential, microstructure, and stress intensity factor on
ALUMINUM ALLOYS AND SYSTEMS/Al- Mo-Sn-Ti-base-Zr, stress corrosion cracking of, effects of electrochemical potential, microstructure, and stress intensity factor on
TIN ALLOYS AND SYSTEMS/ Al-Mo-Sn-Ti-base-Zr, stress corrosion cracking of, effects of electrochemical potential, microstructure, and stress intensity factor on
TITANIUM ALLOYS AND SYSTEMS/Al-Mo-Sn-Ti-base-Zr, stress corrosion cracking of, effects of electrochemical potential, microstructure, and stress intensity factor on
MOLYBDENUM ALLOYS AND SYSTEMS/Al-Mo-Sn-Ti-base-Zr, stress corrosion cracking of, effects of electrochemical potential, microstructure, and stress intensity factor on