SOME INVESTIGATIONS INTO THE STRESS CORROSION BEHAVIOR OF Fe--Ni--Cr ALLOYS IN HIGH TEMPERATURE WATER.
Journal Article
·
· 17p. of Conference Cycle on Chemistry of Water and Aqueous Corrosion in Steam Generators (Conventional and Nuclear). Ecuelles, France Electricite de France (1972).
OSTI ID:4588537
- Research Organization:
- Originating Research Org. not identified
- NSA Number:
- NSA-27-005622
- OSTI ID:
- 4588537
- Journal Information:
- 17p. of Conference Cycle on Chemistry of Water and Aqueous Corrosion in Steam Generators (Conventional and Nuclear). Ecuelles, France Electricite de France (1972)., Other Information: From Conference cycle on chemistry of water and aqueous corrosion in steam generators; Ermenonville, France (13 Mar 1972). See CONF-720323. Orig. Receipt Date: 30-JUN-73
- Country of Publication:
- France
- Language:
- English
Similar Records
Investigation of stress corrosion cracking susceptibility of Fe--Ni--Cr alloys in nuclear reactor water environments.
Corrosion resistance of Ni--Cr stainless steel in high temperature flowing water-corrosion and stress corrosion cracking behavior in high temperature water
Corrosion resistance of Ni--Cr stainless steel in high-temperature flowing water: corrosion and stress-corrosion-cracking behavior in high-temperature water
Journal Article
·
Mon Jan 01 00:00:00 EST 1973
· Corrosion 29: No. 1, 1-12(Jan 1973).
·
OSTI ID:4588537
Corrosion resistance of Ni--Cr stainless steel in high temperature flowing water-corrosion and stress corrosion cracking behavior in high temperature water
Technical Report
·
Wed Oct 31 00:00:00 EST 1973
·
OSTI ID:4588537
+1 more
Corrosion resistance of Ni--Cr stainless steel in high-temperature flowing water: corrosion and stress-corrosion-cracking behavior in high-temperature water
Book
·
Sat Jan 01 00:00:00 EST 1972
·
OSTI ID:4588537
+1 more
Related Subjects
N50210* -Metals
Ceramics
& Other Materials-Metals & Alloys-Corrosion & Erosion & Surface Phenomena
AIR
CHROMIUM
CHROMIUM-NICKEL STEELS
CORROSION RESISTANCE
CRACKS
HIGH TEMPERATURE
LEAD
MATERIALS TESTING
PWR TYPE REACTORS
SOLUTIONS
STEAM GENERATORS
STRESS CORROSION
WATER
NICKEL ALLOYS AND SYSTEMS/Cr-Fe-Ni
stress corrosion by water at 300$sup 0$C
testing for
WATER/corrosive effects on chromium-iron- nickel alloy 600 at 300-C
CHROMIUM ALLOYS AND SYSTEMS/Cr-Fe-Ni
stress corrosion by water at 300$sup 0$C
testing for
IRON ALLOYS AND SYSTEMS/Cr-Fe- Ni
stress corrosion by water at 300$sup 0$C
testing for
Ceramics
& Other Materials-Metals & Alloys-Corrosion & Erosion & Surface Phenomena
AIR
CHROMIUM
CHROMIUM-NICKEL STEELS
CORROSION RESISTANCE
CRACKS
HIGH TEMPERATURE
LEAD
MATERIALS TESTING
PWR TYPE REACTORS
SOLUTIONS
STEAM GENERATORS
STRESS CORROSION
WATER
NICKEL ALLOYS AND SYSTEMS/Cr-Fe-Ni
stress corrosion by water at 300$sup 0$C
testing for
WATER/corrosive effects on chromium-iron- nickel alloy 600 at 300-C
CHROMIUM ALLOYS AND SYSTEMS/Cr-Fe-Ni
stress corrosion by water at 300$sup 0$C
testing for
IRON ALLOYS AND SYSTEMS/Cr-Fe- Ni
stress corrosion by water at 300$sup 0$C
testing for