Title: A STUDY OF THE EFFECTS OF FABRICATING CONDITIONS ON SOME PROPERTIES OF SINTERED URANIUM MONOCARBIDE

Abstract

The effect of initial particle size (6.2 and 14.7 mu ), forming pressure (50,000 and 100,000 psi), temperature (1600 and 1800 deg C), and time at temperature (1 and 3 hr) on the bulk density, grain size, and porosity of sintered uranium monocarbide compacts was studied, Within the limits of the variables studied there appeared to be no significant changes in these properties of the sintered material attributable to the changes in the fabricating conditions. (auth)

Authors:
; ;
Publication Date:
Research Org.:
Battelle Memorial Inst., Columbus, Ohio
OSTI Identifier:
4226895
Report Number(s):
BMI-1383
NSA Number:
NSA-14-001836
DOE Contract Number:  
W-7405-ENG-92
Resource Type:
Technical Report
Resource Relation:
Other Information: Orig. Receipt Date: 31-DEC-60
Country of Publication:
United States
Language:
English
Subject:
METALS, CERAMICS, AND MATERIALS; DENSITY; FABRICATION; GRAIN SIZE; HIGH TEMPERATURE; POROSITY; PRESSURE; SINTERED MATERIALS; URANIUM CARBIDES; VARIATIONS

Citation Formats

Tripler, A.B. Jr., Snyder, M.J., and Duckworth, W.H. A STUDY OF THE EFFECTS OF FABRICATING CONDITIONS ON SOME PROPERTIES OF SINTERED URANIUM MONOCARBIDE. United States: N. p., 1959. Web. doi:10.2172/4226895.
Tripler, A.B. Jr., Snyder, M.J., & Duckworth, W.H. A STUDY OF THE EFFECTS OF FABRICATING CONDITIONS ON SOME PROPERTIES OF SINTERED URANIUM MONOCARBIDE. United States. doi:10.2172/4226895.
Tripler, A.B. Jr., Snyder, M.J., and Duckworth, W.H. Thu . "A STUDY OF THE EFFECTS OF FABRICATING CONDITIONS ON SOME PROPERTIES OF SINTERED URANIUM MONOCARBIDE". United States. doi:10.2172/4226895. https://www.osti.gov/servlets/purl/4226895.
@article{osti_4226895,
title = {A STUDY OF THE EFFECTS OF FABRICATING CONDITIONS ON SOME PROPERTIES OF SINTERED URANIUM MONOCARBIDE},
author = {Tripler, A.B. Jr. and Snyder, M.J. and Duckworth, W.H.},
abstractNote = {The effect of initial particle size (6.2 and 14.7 mu ), forming pressure (50,000 and 100,000 psi), temperature (1600 and 1800 deg C), and time at temperature (1 and 3 hr) on the bulk density, grain size, and porosity of sintered uranium monocarbide compacts was studied, Within the limits of the variables studied there appeared to be no significant changes in these properties of the sintered material attributable to the changes in the fabricating conditions. (auth)},
doi = {10.2172/4226895},
journal = {},
number = ,
volume = ,
place = {United States},
year = {1959},
month = {10}
}