Title: STRESS CORROSION CRACKING OF Ti--8Al--1Mo--1V ALLOY: ELECTROCHEMICAL BEHAVIOR IN AQUEOUS SOLUTIONS.

Journal Article · · Corrosion 26: 135-40(Apr 1970).

Research Organization:
Air Force Materials Lab., Wright-Patterson AFB, Ohio
Sponsoring Organization:
USDOE
NSA Number:
NSA-24-032381
OSTI ID:
4134209
Journal Information:
Corrosion 26: 135-40(Apr 1970)., Other Information: Orig. Receipt Date: 31-DEC-70