Title: Engineering the mechanical properties of ultrabarrier films grown by atomic layer deposition for the encapsulation of printed electronics

Abstract

Direct deposition of barrier films by atomic layer deposition (ALD) onto printed electronics presents a promising method for packaging devices. Films made by ALD have been shown to possess desired ultrabarrier properties, but face challenges when directly grown onto surfaces with varying composition and topography. Challenges include differing nucleation and growth rates across the surface, stress concentrations from topography and coefficient of thermal expansion mismatch, elastic constant mismatch, and particle contamination that may impact the performance of the ALD barrier. In such cases, a polymer smoothing layer may be needed to coat the surface prior to ALD barrier film deposition. We present the impact of architecture on the performance of aluminum oxide (Al{sub 2}O{sub 3})/hafnium oxide (HfO{sub 2}) ALD nanolaminate barrier films deposited on fluorinated polymer layer using an optical calcium (Ca) test under damp heat. It is found that with increasing polymer thickness, the barrier films with residual tensile stress are prone to cracking resulting in rapid failure of the Ca sensor at 50 °C/85% relative humidity. Inserting a SiN{sub x} layer with residual compressive stress between the polymer and ALD layers is found to prevent cracking over a range of polymer thicknesses with more than 95% of the Camore » sensor remaining after 500 h of testing. These results suggest that controlling mechanical properties and film architecture play an important role in the performance of direct deposited ALD barriers.« less

Authors:
; ;  [1]; ; ; ;  [2];  [3]
  1. Woodruff School of Mechanical Engineering, Georgia Institute of Technology, Atlanta, Georgia 30332 (United States)
  2. School of Electrical and Computer Engineering, Georgia Institute of Technology, and Center for Organic Photonics and Electronics, Atlanta, Georgia 30332 (United States)
  3. Oak Ridge National Laboratory, P.O. Box 2008 MS-6064, Oak Ridge, Tennessee 37831 (United States)
Publication Date:
OSTI Identifier:
22494811
Resource Type:
Journal Article
Journal Name:
Journal of Applied Physics
Additional Journal Information:
Journal Volume: 118; Journal Issue: 8; Other Information: (c) 2015 AIP Publishing LLC; Country of input: International Atomic Energy Agency (IAEA); Journal ID: ISSN 0021-8979
Country of Publication:
United States
Language:
English
Subject:
36 MATERIALS SCIENCE; ALUMINIUM OXIDES; CALCIUM; CONTAMINATION; CRACKS; DEPOSITION; DIFFUSION BARRIERS; ENCAPSULATION; HAFNIUM OXIDES; HUMIDITY; MECHANICAL PROPERTIES; NUCLEATION; POLYMERS; PRINTED CIRCUITS; SENSORS; STRESSES; THERMAL EXPANSION; THIN FILMS; TOPOGRAPHY

Citation Formats

Bulusu, A., Singh, A., Kim, H., Wang, C. Y., Dindar, A., Fuentes-Hernandez, C., Kippelen, B., Cullen, D., Graham, S., E-mail: sgraham@gatech.edu, and Oak Ridge National Laboratory, P.O. Box 2008 MS-6064, Oak Ridge, Tennessee 37831. Engineering the mechanical properties of ultrabarrier films grown by atomic layer deposition for the encapsulation of printed electronics. United States: N. p., 2015. Web. doi:10.1063/1.4928855.
Bulusu, A., Singh, A., Kim, H., Wang, C. Y., Dindar, A., Fuentes-Hernandez, C., Kippelen, B., Cullen, D., Graham, S., E-mail: sgraham@gatech.edu, & Oak Ridge National Laboratory, P.O. Box 2008 MS-6064, Oak Ridge, Tennessee 37831. Engineering the mechanical properties of ultrabarrier films grown by atomic layer deposition for the encapsulation of printed electronics. United States. doi:10.1063/1.4928855.
Bulusu, A., Singh, A., Kim, H., Wang, C. Y., Dindar, A., Fuentes-Hernandez, C., Kippelen, B., Cullen, D., Graham, S., E-mail: sgraham@gatech.edu, and Oak Ridge National Laboratory, P.O. Box 2008 MS-6064, Oak Ridge, Tennessee 37831. Fri . "Engineering the mechanical properties of ultrabarrier films grown by atomic layer deposition for the encapsulation of printed electronics". United States. doi:10.1063/1.4928855.
@article{osti_22494811,
title = {Engineering the mechanical properties of ultrabarrier films grown by atomic layer deposition for the encapsulation of printed electronics},
author = {Bulusu, A. and Singh, A. and Kim, H. and Wang, C. Y. and Dindar, A. and Fuentes-Hernandez, C. and Kippelen, B. and Cullen, D. and Graham, S., E-mail: sgraham@gatech.edu and Oak Ridge National Laboratory, P.O. Box 2008 MS-6064, Oak Ridge, Tennessee 37831},
abstractNote = {Direct deposition of barrier films by atomic layer deposition (ALD) onto printed electronics presents a promising method for packaging devices. Films made by ALD have been shown to possess desired ultrabarrier properties, but face challenges when directly grown onto surfaces with varying composition and topography. Challenges include differing nucleation and growth rates across the surface, stress concentrations from topography and coefficient of thermal expansion mismatch, elastic constant mismatch, and particle contamination that may impact the performance of the ALD barrier. In such cases, a polymer smoothing layer may be needed to coat the surface prior to ALD barrier film deposition. We present the impact of architecture on the performance of aluminum oxide (Al{sub 2}O{sub 3})/hafnium oxide (HfO{sub 2}) ALD nanolaminate barrier films deposited on fluorinated polymer layer using an optical calcium (Ca) test under damp heat. It is found that with increasing polymer thickness, the barrier films with residual tensile stress are prone to cracking resulting in rapid failure of the Ca sensor at 50 °C/85% relative humidity. Inserting a SiN{sub x} layer with residual compressive stress between the polymer and ALD layers is found to prevent cracking over a range of polymer thicknesses with more than 95% of the Ca sensor remaining after 500 h of testing. These results suggest that controlling mechanical properties and film architecture play an important role in the performance of direct deposited ALD barriers.},
doi = {10.1063/1.4928855},
journal = {Journal of Applied Physics},
issn = {0021-8979},
number = 8,
volume = 118,
place = {United States},
year = {2015},
month = {8}
}