Title: Analysis of scattering mechanisms in zinc oxide films grown by the atomic layer deposition technique

Journal Article · · Journal of Applied Physics
DOI:https://doi.org/10.1063/1.4927294· OSTI ID:22489537
; ; ; ; ;  [1];  [1]
  1. Institute of Physics, Polish Academy of Sciences, Al. Lotnikow 32/46, 02-668 Warsaw (Poland)

In this work, the analysis of the temperature-dependent electrical conductivity of highly crystalline zinc oxide (ZnO) thin films obtained by the Atomic Layer Deposition (ALD) method is performed. It is deduced that the most important scattering mechanisms are: scattering by ionized defects (at low temperatures) as well as by phonons (mainly optical ones) at higher temperatures. Nevertheless, the role of grain boundaries in the carrier mobility limitation ought to be included as well. These conclusions are based on theoretical analysis and temperature-dependent Hall mobility measurements. The presented results prove that existing models can explain the mobility behavior in the ALD-ZnO films, being helpful for understanding their transport properties, which are strongly related both to the crystalline quality of deposited ZnO material and defects in its lattice.

OSTI ID:
22489537
Journal Information:
Journal of Applied Physics, Vol. 118, Issue 3; Other Information: (c) 2015 AIP Publishing LLC; Country of input: International Atomic Energy Agency (IAEA); ISSN 0021-8979
Country of Publication:
United States
Language:
English

Similar Records

Effect of in situ hydrogen plasma treatment on zinc oxide grown using low temperature atomic layer deposition
Journal Article · Tue Jan 15 00:00:00 EST 2013 · Journal of Vacuum Science and Technology. A, Vacuum, Surfaces and Films · OSTI ID:22489537

Impact of surface morphology of Si substrate on performance of Si/ZnO heterojunction devices grown by atomic layer deposition technique
Journal Article · Thu Jan 01 00:00:00 EST 2015 · Journal of Vacuum Science and Technology. A, Vacuum, Surfaces and Films · OSTI ID:22489537

A revisit to atomic layer deposition of zinc oxide using diethylzinc and water as precursors
Journal Article · Wed Dec 19 00:00:00 EST 2018 · Journal of Materials Science · OSTI ID:22489537