Title: Atomic force microscopy based nanoindentation study of onion abaxial epidermis walls in aqueous environment

Abstract

An atomic force microscopy based nanoindentation method was employed to study how the structure of cellulose microfibril packing and matrix polymers affect elastic modulus of fully hydrated primary plant cell walls. The isolated, single-layered abaxial epidermis cell wall of an onion bulb was used as a test system since the cellulose microfibril packing in this cell wall is known to vary systematically from inside to outside scales and the most abundant matrix polymer, pectin, can easily be altered through simple chemical treatments such as ethylenediaminetetraacetic acid and calcium ions. Experimental results showed that the pectin network variation has significant impacts on the cell wall modulus, and not the cellulose microfibril packing.

Authors:
;  [1];  [2]
  1. Department of Engineering Science and Mechanics, Pennsylvania State University, University Park, Pennsylvania 16802 (United States)
  2. Department of Chemical Engineering, Pennsylvania State University, University Park, Pennsylvania 16802 (United States)
Publication Date:
OSTI Identifier:
22412839
Resource Type:
Journal Article
Resource Relation:
Journal Name: Journal of Applied Physics; Journal Volume: 117; Journal Issue: 2; Other Information: (c) 2015 AIP Publishing LLC; Country of input: International Atomic Energy Agency (IAEA)
Country of Publication:
United States
Language:
English
Subject:
36 MATERIALS SCIENCE; ATOMIC FORCE MICROSCOPY; CALCIUM IONS; CELL WALL; CELLULOSE; EDTA; ELASTICITY; EPIDERMIS; PECTINS; POLYMERS; VARIATIONS; YOUNG MODULUS

Citation Formats

Xi, Xiaoning, Tittmann, Bernhard, and Kim, Seong H. Atomic force microscopy based nanoindentation study of onion abaxial epidermis walls in aqueous environment. United States: N. p., 2015. Web. doi:10.1063/1.4906094.
Xi, Xiaoning, Tittmann, Bernhard, & Kim, Seong H. Atomic force microscopy based nanoindentation study of onion abaxial epidermis walls in aqueous environment. United States. doi:10.1063/1.4906094.
Xi, Xiaoning, Tittmann, Bernhard, and Kim, Seong H. Wed . "Atomic force microscopy based nanoindentation study of onion abaxial epidermis walls in aqueous environment". United States. doi:10.1063/1.4906094.
@article{osti_22412839,
title = {Atomic force microscopy based nanoindentation study of onion abaxial epidermis walls in aqueous environment},
author = {Xi, Xiaoning and Tittmann, Bernhard and Kim, Seong H.},
abstractNote = {An atomic force microscopy based nanoindentation method was employed to study how the structure of cellulose microfibril packing and matrix polymers affect elastic modulus of fully hydrated primary plant cell walls. The isolated, single-layered abaxial epidermis cell wall of an onion bulb was used as a test system since the cellulose microfibril packing in this cell wall is known to vary systematically from inside to outside scales and the most abundant matrix polymer, pectin, can easily be altered through simple chemical treatments such as ethylenediaminetetraacetic acid and calcium ions. Experimental results showed that the pectin network variation has significant impacts on the cell wall modulus, and not the cellulose microfibril packing.},
doi = {10.1063/1.4906094},
journal = {Journal of Applied Physics},
number = 2,
volume = 117,
place = {United States},
year = {Wed Jan 14 00:00:00 EST 2015},
month = {Wed Jan 14 00:00:00 EST 2015}
}