Abstract

Zirconium nitride (ZrN) has the lowest bulk electrical resistivity and high thermal stability among group IV and V transition metal nitrides, which makes it a promising material for ULSI applications such as a diffusion barrier for Cu interconnects, contact metal in III-V semiconductor devices, and in high density memory structures. Plasma enhanced atomic layer deposition (PEALD) of conducting ZrN thin films using Zr[N(CH{sub 3}){sub 2}]{sub 4} and forming gas (5% H{sub 2} + 95% N{sub 2}) plasma is reported in this article. The growth per cycle (GPC) for every deposition was determined from analysis of dynamic in-situ spectroscopic ellipsometry (d-iSE) measurements. An experimental design is proposed for faster determination of ALD growth saturation curves. At substrate temperature of 150 °C, a GPC of 0.10 nm/cycle was observed for self-limiting ZrN PEALD growth. The electrical resistivity of ZrN films deposited on SiO{sub 2} substrate was found to be 559.5 ± 18.5 μΩ cm with negligible change in resistivity even after ∼1000 h exposure to air. The metallic behavior of our ZrN films was evident from the free electron dispersion component in dielectric response, the broad band of photoelectron emission across Fermi level and the positive temperature coefficient for resistivity of 0.0088/ °C.

Authors:
;  [1]
  1. Department of Chemical and Materials Engineering, University of Alberta, Edmonton, Alberta T6G 2V4 (Canada)
Publication Date:
OSTI Identifier:
22392176
Resource Type:
Journal Article
Journal Name:
Journal of Vacuum Science and Technology. A, Vacuum, Surfaces and Films
Additional Journal Information:
Journal Volume: 33; Journal Issue: 3; Other Information: (c) 2015 American Vacuum Society; Country of input: International Atomic Energy Agency (IAEA); Journal ID: ISSN 0734-2101
Country of Publication:
United States
Language:
English
Subject:
36 MATERIALS SCIENCE; DENSITY; DEPOSITION; DEPOSITS; DIELECTRIC MATERIALS; ELECTRIC CONDUCTIVITY; ELLIPSOMETRY; FERMI LEVEL; PLASMA; SILICA; SILICON OXIDES; SUBSTRATES; TEMPERATURE COEFFICIENT; THIN FILMS; ZIRCONIUM NITRIDES

Citation Formats

Muneshwar, Triratna, E-mail: muneshwa@ualberta.ca, and Cadien, Ken. Low temperature plasma enhanced atomic layer deposition of conducting zirconium nitride films using tetrakis (dimethylamido) zirconium and forming gas (5% H{sub 2} + 95% N{sub 2}) plasma. United States: N. p., 2015. Web. doi:10.1116/1.4915122.
Muneshwar, Triratna, E-mail: muneshwa@ualberta.ca, & Cadien, Ken. Low temperature plasma enhanced atomic layer deposition of conducting zirconium nitride films using tetrakis (dimethylamido) zirconium and forming gas (5% H{sub 2} + 95% N{sub 2}) plasma. United States. doi:10.1116/1.4915122.
Muneshwar, Triratna, E-mail: muneshwa@ualberta.ca, and Cadien, Ken. Fri . "Low temperature plasma enhanced atomic layer deposition of conducting zirconium nitride films using tetrakis (dimethylamido) zirconium and forming gas (5% H{sub 2} + 95% N{sub 2}) plasma". United States. doi:10.1116/1.4915122.
@article{osti_22392176,
title = {Low temperature plasma enhanced atomic layer deposition of conducting zirconium nitride films using tetrakis (dimethylamido) zirconium and forming gas (5% H{sub 2} + 95% N{sub 2}) plasma},
author = {Muneshwar, Triratna, E-mail: muneshwa@ualberta.ca and Cadien, Ken},
abstractNote = {Zirconium nitride (ZrN) has the lowest bulk electrical resistivity and high thermal stability among group IV and V transition metal nitrides, which makes it a promising material for ULSI applications such as a diffusion barrier for Cu interconnects, contact metal in III-V semiconductor devices, and in high density memory structures. Plasma enhanced atomic layer deposition (PEALD) of conducting ZrN thin films using Zr[N(CH{sub 3}){sub 2}]{sub 4} and forming gas (5% H{sub 2} + 95% N{sub 2}) plasma is reported in this article. The growth per cycle (GPC) for every deposition was determined from analysis of dynamic in-situ spectroscopic ellipsometry (d-iSE) measurements. An experimental design is proposed for faster determination of ALD growth saturation curves. At substrate temperature of 150 °C, a GPC of 0.10 nm/cycle was observed for self-limiting ZrN PEALD growth. The electrical resistivity of ZrN films deposited on SiO{sub 2} substrate was found to be 559.5 ± 18.5 μΩ cm with negligible change in resistivity even after ∼1000 h exposure to air. The metallic behavior of our ZrN films was evident from the free electron dispersion component in dielectric response, the broad band of photoelectron emission across Fermi level and the positive temperature coefficient for resistivity of 0.0088/ °C.},
doi = {10.1116/1.4915122},
journal = {Journal of Vacuum Science and Technology. A, Vacuum, Surfaces and Films},
issn = {0734-2101},
number = 3,
volume = 33,
place = {United States},
year = {2015},
month = {5}
}