Abstract

In this paper, the authors demonstrate a novel spatial atomic layer deposition (ALD) process based on pneumatic transport of nanoparticle agglomerates. Nanoclusters of platinum (Pt) of ∼1 nm diameter are deposited onto titania (TiO{sub 2}) P25 nanoparticles resulting to a continuous production of an active photocatalyst (0.12–0.31 wt. % of Pt) at a rate of about 1 g min{sup −1}. Tuning the precursor injection velocity (10–40 m s{sup −1}) enhances the contact between the precursor and the pneumatically transported support flows. Decreasing the chemisorption temperature (from 250 to 100 °C) results in more uniform distribution of the Pt nanoclusters as it decreases the reaction rate as compared to the rate of diffusion into the nanoparticle agglomerates. Utilizing this photocatalyst in the oxidation reaction of Acid Blue 9 showed a factor of five increase of the photocatalytic activity compared to the native P25 nanoparticles. The use of spatial particle ALD can be further expanded to deposition of nanoclusters on porous, micron-sized particles and to the production of core–shell nanoparticles enabling the robust and scalable manufacturing of nanostructured powders for catalysis and other applications.

Authors:
; ; ; ;  [1]
  1. Department of Chemical Engineering, Delft University of Technology, Julianalaan 136, 2628 BL Delft (Netherlands)
Publication Date:
OSTI Identifier:
22392158
Resource Type:
Journal Article
Resource Relation:
Journal Name: Journal of Vacuum Science and Technology. A, Vacuum, Surfaces and Films; Journal Volume: 33; Journal Issue: 2; Other Information: (c) 2015 American Vacuum Society; Country of input: International Atomic Energy Agency (IAEA)
Country of Publication:
United States
Language:
English
Subject:
37 INORGANIC, ORGANIC, PHYSICAL AND ANALYTICAL CHEMISTRY; CHEMISORPTION; DEPOSITION; DEPOSITS; MANUFACTURING; NANOPARTICLES; NANOSTRUCTURES; PHOTOCATALYSIS; PNEUMATIC TRANSPORT; POROUS MATERIALS; REACTION KINETICS; TITANIUM OXIDES

Citation Formats

Ommen, J. Ruud van, E-mail: j.r.vanommen@tudelft.nl, Kooijman, Dirkjan, Niet, Mark de, Talebi, Mojgan, and Goulas, Aristeidis. Continuous production of nanostructured particles using spatial atomic layer deposition. United States: N. p., 2015. Web. doi:10.1116/1.4905725.
Ommen, J. Ruud van, E-mail: j.r.vanommen@tudelft.nl, Kooijman, Dirkjan, Niet, Mark de, Talebi, Mojgan, & Goulas, Aristeidis. Continuous production of nanostructured particles using spatial atomic layer deposition. United States. doi:10.1116/1.4905725.
Ommen, J. Ruud van, E-mail: j.r.vanommen@tudelft.nl, Kooijman, Dirkjan, Niet, Mark de, Talebi, Mojgan, and Goulas, Aristeidis. Sun . "Continuous production of nanostructured particles using spatial atomic layer deposition". United States. doi:10.1116/1.4905725.
@article{osti_22392158,
title = {Continuous production of nanostructured particles using spatial atomic layer deposition},
author = {Ommen, J. Ruud van, E-mail: j.r.vanommen@tudelft.nl and Kooijman, Dirkjan and Niet, Mark de and Talebi, Mojgan and Goulas, Aristeidis},
abstractNote = {In this paper, the authors demonstrate a novel spatial atomic layer deposition (ALD) process based on pneumatic transport of nanoparticle agglomerates. Nanoclusters of platinum (Pt) of ∼1 nm diameter are deposited onto titania (TiO{sub 2}) P25 nanoparticles resulting to a continuous production of an active photocatalyst (0.12–0.31 wt. % of Pt) at a rate of about 1 g min{sup −1}. Tuning the precursor injection velocity (10–40 m s{sup −1}) enhances the contact between the precursor and the pneumatically transported support flows. Decreasing the chemisorption temperature (from 250 to 100 °C) results in more uniform distribution of the Pt nanoclusters as it decreases the reaction rate as compared to the rate of diffusion into the nanoparticle agglomerates. Utilizing this photocatalyst in the oxidation reaction of Acid Blue 9 showed a factor of five increase of the photocatalytic activity compared to the native P25 nanoparticles. The use of spatial particle ALD can be further expanded to deposition of nanoclusters on porous, micron-sized particles and to the production of core–shell nanoparticles enabling the robust and scalable manufacturing of nanostructured powders for catalysis and other applications.},
doi = {10.1116/1.4905725},
journal = {Journal of Vacuum Science and Technology. A, Vacuum, Surfaces and Films},
number = 2,
volume = 33,
place = {United States},
year = {Sun Mar 15 00:00:00 EDT 2015},
month = {Sun Mar 15 00:00:00 EDT 2015}
}