Title: Characterization of ZnO film grown on polycarbonate by atomic layer deposition at low temperature

Abstract

ZnO is an attractive material for use in various technological products such as phosphors, gas sensors, and transparent conductors. Recently, aluminum-doped zinc oxide has received attention as a potential replacement for indium tin oxide, which is one of the transparent conductive oxides used in flat panel displays, organic light-emitting diodes, and organic solar cells. In this study, the characteristics of ZnO films deposited on polycarbonate (PC) substrates by atomic layer deposition (ALD) are investigated for various process temperatures. The growth mechanism of these films was investigated at low process temperatures using x-ray diffraction (XRD) and x-ray photoelectron spectroscopy (XPS). XRD and XPS were used to determine the preferred orientation and chemical composition of the films, respectively. Furthermore, the difference of the deposition mechanisms on an amorphous organic material, i.e., PC substrate and an inorganic material such as silicon was discussed from the viewpoint of the diffusion and deposition of precursors. The structure of the films was also investigated by chemical analysis in order to determine the effect of growth temperature on the films deposited by ALD.

Authors:
; ; ;  [1]
  1. School of Mechanical Engineering, Korea University, Seoul 136-707 (Korea, Republic of)
Publication Date:
OSTI Identifier:
22392107
Resource Type:
Journal Article
Resource Relation:
Journal Name: Journal of Vacuum Science and Technology. A, Vacuum, Surfaces and Films; Journal Volume: 33; Journal Issue: 1; Other Information: (c) 2014 American Vacuum Society; Country of input: International Atomic Energy Agency (IAEA)
Country of Publication:
United States
Language:
English
Subject:
36 MATERIALS SCIENCE; ALUMINIUM; CHEMICAL ANALYSIS; CHEMICAL COMPOSITION; DEPOSITION; DOPED MATERIALS; FILMS; GRAIN ORIENTATION; POLYCARBONATES; SUBSTRATES; TIN OXIDES; X-RAY DIFFRACTION; X-RAY PHOTOELECTRON SPECTROSCOPY; ZINC OXIDES

Citation Formats

Lee, Gyeong Beom, Han, Gwon Deok, Shim, Joon Hyung, and Choi, Byoung-Ho, E-mail: bhchoi@korea.ac.kr. Characterization of ZnO film grown on polycarbonate by atomic layer deposition at low temperature. United States: N. p., 2015. Web. doi:10.1116/1.4903270.
Lee, Gyeong Beom, Han, Gwon Deok, Shim, Joon Hyung, & Choi, Byoung-Ho, E-mail: bhchoi@korea.ac.kr. Characterization of ZnO film grown on polycarbonate by atomic layer deposition at low temperature. United States. doi:10.1116/1.4903270.
Lee, Gyeong Beom, Han, Gwon Deok, Shim, Joon Hyung, and Choi, Byoung-Ho, E-mail: bhchoi@korea.ac.kr. Thu . "Characterization of ZnO film grown on polycarbonate by atomic layer deposition at low temperature". United States. doi:10.1116/1.4903270.
@article{osti_22392107,
title = {Characterization of ZnO film grown on polycarbonate by atomic layer deposition at low temperature},
author = {Lee, Gyeong Beom and Han, Gwon Deok and Shim, Joon Hyung and Choi, Byoung-Ho, E-mail: bhchoi@korea.ac.kr},
abstractNote = {ZnO is an attractive material for use in various technological products such as phosphors, gas sensors, and transparent conductors. Recently, aluminum-doped zinc oxide has received attention as a potential replacement for indium tin oxide, which is one of the transparent conductive oxides used in flat panel displays, organic light-emitting diodes, and organic solar cells. In this study, the characteristics of ZnO films deposited on polycarbonate (PC) substrates by atomic layer deposition (ALD) are investigated for various process temperatures. The growth mechanism of these films was investigated at low process temperatures using x-ray diffraction (XRD) and x-ray photoelectron spectroscopy (XPS). XRD and XPS were used to determine the preferred orientation and chemical composition of the films, respectively. Furthermore, the difference of the deposition mechanisms on an amorphous organic material, i.e., PC substrate and an inorganic material such as silicon was discussed from the viewpoint of the diffusion and deposition of precursors. The structure of the films was also investigated by chemical analysis in order to determine the effect of growth temperature on the films deposited by ALD.},
doi = {10.1116/1.4903270},
journal = {Journal of Vacuum Science and Technology. A, Vacuum, Surfaces and Films},
number = 1,
volume = 33,
place = {United States},
year = {Thu Jan 15 00:00:00 EST 2015},
month = {Thu Jan 15 00:00:00 EST 2015}
}